Answers for choosing, setting up and using a small air-cooled micro TIG torch for tight-access work.
What is a micro TIG torch and when is it worth using?

A micro TIG torch has a very small, lightweight head and body that gives pen-like control. It is aimed at thin material and joints where a standard torch head is simply too bulky to reach, such as inside frames, small fabrications, aerospace-style repair work and fine decorative metalwork.
The smaller head usually means a lower current rating than a full-size torch, so it suits light-duty, precise work rather than heavy sections. Check the rating on the torch and in the maker's manual against the current you need before buying.
Why would I choose a clear glass cup, and what are the drawbacks?

A clear heat-resistant glass cup lets you see through the cup to the weld pool and the tungsten, which gives better control in corners and awkward joints. On a micro torch the small head already helps access, and the clear cup adds visibility of the joint.
The drawbacks are that glass can chip or crack if knocked or dropped, and glass cups are not well suited to walking the cup along the joint. Larger cups and longer stick-out also reduce the visibility benefit. Many welders keep a few ceramic cups as well for rougher work.
How should I set the tungsten stick-out on a micro torch?

Stick-out is how far the tungsten extends beyond the cup. A longer stick-out helps reach tight spots because it moves the arc away from the bulky cup, but the usual rule is that the larger the cup, the longer the stick-out can be.
On a small cup keep the stick-out as short as access allows, and do not extend it further than you need. With a longer stick-out, allow plenty of gas pre-flow, because argon is heavier than air and the shielding can be disturbed. Check for a clean, bright weld with no discolouration, and follow your torch and machine manuals.
Should I choose an air-cooled or a water-cooled micro torch?

Air-cooled torches rely on the surrounding air and the shielding gas to carry heat away. They are simpler, need no separate cooling unit, and suit light-duty, shorter welding runs and lower currents.
Water-cooled torches are connected to a separate cooling unit. They have a higher duty cycle, so they last longer before heating up, and are the better choice for higher current or long continuous welding. Their cables are often lighter and more flexible. Duty cycle is measured over ten minutes, so a 60% rating means about six minutes of welding and four minutes of cooling. Use the torch at or below its rated current, and see the maker's data plate.
Which tungsten electrode suits low-current work on a micro torch?

Small electrodes are used on a micro torch because the current is low. Ceriated tungsten is popular for small, delicate work because it starts well at low current, and lanthanated electrodes behave in a similar way to thoriated ones, so they are a common replacement.
Thoriated tungsten contains low levels of radioactivity, so if you grind it you should control and collect the dust and have adequate ventilation at the grinding station. Always follow the electrode maker's safety data sheet. Match the electrode diameter to the current and to your collet and collet body.
Do I need to worry about ozone and fume when TIG welding in tight spaces?

Yes. The HSE says that ozone in particular can cause throat dryness, coughing or chest tightness when TIG welding stainless steel and aluminium, and welding fume more generally can harm health. Tight, enclosed work tends to make fume harder to clear.
The HSE recommends capturing fume at source with local exhaust ventilation, with respiratory protective equipment where that alone is not enough. Your employer's COSHH assessment should decide the right controls for the material, the work and how often you weld.
What gas flow should I use with a small cup?

A common starting rule is to use a flow in litres per minute roughly equal to the cup number, which reflects the cup's inner diameter in sixteenths of an inch. Small cups therefore need modest flow.
Too much flow can make the arc unstable and draw air in, while too little leaves the weld unprotected. Draughts reduce shielding and can cause porosity and inclusions. Start low, check the weld for a clean finish, and follow the guidance in your machine and torch manuals.