ATO Fast Purge

This multi-sized system makes an effective seal for purging pipework across a wide range of pipe diameters. Each Purge system covers multiple pipe sizes and schedules, so you need fewer systems.

Professional, robust solution for purging of stainless steel, duplex and other alloy pipework, resulting in shiny, oxide-free weld roots. Plug and purge: connect to a dedicated and regulated gas supply and choose any flow rate, up to 80 litres per minute, through the pre-set purge valve. Setup times are dramatically reduced. Lower gas volumes are required, reducing costs. Heat-resistant up to 250°c. Lightweight and collapsible, patented design manufactured in the UK.

ATO Fast Purge FAQs

Answers on choosing and using multi-size inflatable purge systems that cover a range of pipe diameters.

What is a multi-size inflatable purge system?icon-minus-redicon-plus-red

It is a twin-dam inflatable purge system designed so that one unit seals across a range of pipe bores, rather than being made for a single pipe size. The dams inflate against the pipe wall to enclose a short length around the joint, and purge gas then fills the space between them to displace the air.

The aim is to need fewer systems to cover your pipe sizes and wall thicknesses. The bore range for each unit is stated by the maker, so check that your pipe falls within it before buying.

How do I decide between small, medium and large bore versions?icon-minus-redicon-plus-red

Each version covers a band of pipe bore sizes, and the bands are set by the maker. Start by finding the inside diameter of the pipe you weld most often, then pick the version whose stated range contains it. If you weld across more than one band, you will usually need more than one system.

If your bore sits right at the edge of a range, check with the supplier or the maker's chart before choosing, because a bag stretched to its limit may not seal as well as one working mid-range.

How does pipe wall thickness affect which system I need?icon-minus-redicon-plus-red

The outside diameter of a nominal pipe size stays the same, but the wall thickness changes the inside diameter. The inside diameter is the outside diameter minus twice the wall thickness, so a heavier schedule of the same nominal size has a smaller bore.

Because multi-size systems are specified by bore range, work out the actual inside diameter for the schedule or tube you are welding rather than going by nominal size alone, and compare it with the range given in the maker's data.

Do I need a regulated gas supply, and what does a pre-set purge valve do?icon-minus-redicon-plus-red

Yes, use a regulated supply with a suitable flow control rather than connecting the system straight to a cylinder or line. Maker descriptions of these systems say you connect a regulated gas supply, and a pre-set valve controls how gas enters the chamber once the bags have sealed, so you do not have to set it each time.

The maximum flow, the supply pressure and the valve arrangement differ between models, so follow the maker's instructions and data plate. Never raise the supply pressure above what the system is designed for.

Can I turn the flow right up to purge faster?icon-minus-redicon-plus-red

Not without checking the maker's limits. Over-pressure is a known cause of inflatable dam failure, and changes in gas flow made by other people near the work can also over-inflate the bags, particularly as heat from welding builds up.

Use the maximum flow your system is rated for only to flush the air out, then reduce the flow to a gentle level while welding if your procedure calls for it. A burst bag means a lost purge and an oxidised weld.

How does heat affect the system, and how close to the weld can the bags sit?icon-minus-redicon-plus-red

Heat from welding, and from preheat or interpass temperatures, travels along the pipe and can swell or damage inflatable dams. Heat-resistant versions are rated up to a stated temperature, which is a figure for you to check on the maker's data sheet, including whether it is continuous or only for short periods.

The safe distance between the bags and the joint depends on the system, the pipe wall thickness and the heat input, so follow the maker's guidance and keep the bags comfortably away from the hottest zone.

What happens if a bag fails or the purge is interrupted mid-weld?icon-minus-redicon-plus-red

Once a burst occurs, the purge is lost and the hot weld oxidises as soon as air reaches it. Stop welding, shut off the heat, and do not carry on over a contaminated root.

After the pipe cools, inspect the affected area. Whether it can be recovered, cleaned or must be cut out depends on the material, the specification and your welding procedure, so follow the procedure and speak to the person responsible for weld quality. Check the bag for the cause before re-using it.