WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE

MIG ER80S-Ni

Description:

MIG ER80S-Ni is a copper-coated wire depositing a nominal 0.9% Ni weld metal. It has a guaranteed Ni content of 1% maximum, ensuring conformance to NACE requirements for oil and gas production equipment.  The wire is primarily intended for GMAW but is equally suitable for use in mechanised GTAW eg. orbital TIG process (see Elgatig 162 for mechanical properties).

MIG ER80S-Ni gives very good fracture toughness at temperatures down to –60°c and is intended for offshore pipework and similar high-integrity applications.

  C Si Mn P S Cr Ni Mo Cu V Al Ti
Min 0,06 0,50 1,00       0,80          
Typical 0,09 0,60 1,10 0,010 0,010   0,90          
Max 0,12 0,80 1,25 0,020 0,020 0,15 0,99 0,15 0,35 0,03 0,02 0,15



Shielding Gas:
Acc. to EN 439:
C1, 100% CO2, 7-10 l/min.
M21, 80% Ar +20% CO2, 7-10 l/min.

MIG ER80S-Ni FAQs

Straight answers to the questions people ask most when choosing and using nickel-alloyed ER80S-Ni MIG wire.

What is the difference between ER80S-Ni1 and ER80S-Ni2?icon-minus-redicon-plus-red

The main difference is the nickel content. The classification for Ni1 calls for roughly 0.8 to 1.1% nickel, while Ni2 calls for roughly 2 to 2.75%. Higher nickel generally gives better toughness at very low temperatures, so Ni2 is aimed at colder service, while Ni1 suits moderately low temperatures.

Both are in the same 80 ksi strength class. Note that the Ni1 range runs slightly above 1%, so if your specification sets a 1% nickel limit, such as for sour service, check the nickel figure on the batch certificate rather than relying on the class alone. Which wire you need depends on the lowest service temperature, the parent steel and the weld procedure.

Why is the nickel limit of 1% so important for oil and gas work?icon-minus-redicon-plus-red

For sour service, where hydrogen sulphide is present, the sour service standard requires sulphide stress cracking testing for carbon-manganese steel welds with more than 1% nickel in the deposit. Nickel is therefore generally kept to 1% maximum on such work, which is why a wire with a controlled nickel level is chosen.

Some specifications allow a higher figure when it has been specially tested. Whether it applies to your job depends on the project specification and the current edition of the standard, so check those and the wire's certificate rather than assuming.

What does ER80S-Ni mean?icon-minus-redicon-plus-red

It is a classification under the American standard for solid low-alloy steel wire used with gas shielding. The R shows it can be used as a rod or an electrode, the 80 means weld metal of about 80 ksi (550 MPa) minimum tensile strength, and the S means a solid wire. Ni shows that nickel is added deliberately.

The number after Ni, such as Ni1 or Ni2, shows the nickel level band. The wire is made for good toughness at low temperature, so it is used on offshore, pipework and similar demanding jobs. Always check the wire's certificate for the exact class it meets.

When do I need a nickel wire instead of a standard steel wire?icon-minus-redicon-plus-red

A standard mild steel wire is fine for general work, but plain carbon-manganese gas-shielded wires may not give adequate weld metal toughness at low temperatures such as -50 degrees C. Nickel is then usually needed to provide the required as-welded toughness.

Nickel wires are therefore chosen when the specification calls for low-temperature impact toughness, such as offshore structures, pipework and cold-climate equipment. Makers also list them for sour-service work and some weathering steels. If your drawing or welding procedure names the filler, use that. If not, ask the designer or welding engineer.

Do I need to preheat when using ER80S-Ni wire?icon-minus-redicon-plus-red

It depends on the parent steel, thickness, restraint and the hydrogen level of the process. Preheat slows cooling, lets hydrogen escape and reduces hardness, which lowers the risk of hydrogen cracking.

For low carbon-equivalent steels preheat is generally not needed if a low hydrogen process is used, but thick or highly restrained joints may need it, and higher carbon-equivalent steels need it more often. The joint must also be clean and dry. Follow the welding procedure for preheat and interpass temperatures rather than guessing from the wire alone.

Which shielding gas should I use with ER80S-Ni wire?icon-minus-redicon-plus-red

Use the gas listed on the wire's data sheet and in your welding procedure, usually an argon-rich mixture. Gas choice affects arc, spatter, penetration and toughness.

Gas suppliers explain that adding oxygen or carbon dioxide raises the oxidation potential of the gas. For a given wire, the higher that is, the lower the strength and toughness of the weld, because oxide inclusions increase and manganese and silicon are lost. Where impact toughness matters, do not change the gas or flow rate from the approved procedure without checking with the welding engineer.