WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : 1100X  

    UTP DUR 600 Hardfacing Electrodes. E 6-UM-60
    1100X

    Select Option 
    Prices From £49.48 ex VAT

    UTP DUR 600 is universally applicable for cladding on parts of steel, cast steel and high Mn-steel, subject simultaneously to abrasion, impact and compression. Typical application fields are the earth moving and stone treatment industry, e.g. excavator teeth, bucker knives, crusher jaws and cones, mill hammers etc., but also for cutting edges on cold cutting tools. The deposit is machinable by grinding only.

    Standard
    DIN 8555: E 6-UM-60

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Hardfacing Electrodes FAQs

    Straight answers on choosing and using hardfacing electrodes to protect parts from abrasion, impact and wear.

    What is a hardfacing electrode for, and how is it different from an ordinary electrode?icon-minus-redicon-plus-red

    A hardfacing electrode deposits a wear-resistant layer on the surface of a part, either to protect a new part or to rebuild one that has worn. An ordinary electrode is chosen to join two pieces of metal with a deposit that is strong and tough. A hardfacing deposit is chosen to resist wear, so it is usually much harder and often more brittle.

    It extends the life of things like digger teeth, blades, crusher parts and screw conveyors. It is a surface treatment, not a way of joining or strengthening a structure.

    How do I choose the right hardfacing electrode for my wear problem?icon-minus-redicon-plus-red

    Start by working out how the part wears. Sliding of grit, soil or rock across the surface is abrasion. Heavy knocks and blows are impact. Metal rubbing on metal, as in gears, rollers and sprockets, is metal-to-metal wear. Heat or corrosion may also be involved.

    Broadly, deposits rich in chromium carbide are chosen where abrasion dominates and impact is low to moderate. Tougher, more ductile deposits suit heavy impact, and tool-steel type deposits suit metal-to-metal wear. The hardest deposit is not always the best, because very hard deposits tend to be brittle. Check the maker's data sheet for what each electrode is designed to resist, and tell us the part and the wear if you would like help choosing.

    Can I hardface manganese steel?icon-minus-redicon-plus-red

    Take care. Austenitic manganese steel, commonly used for digger teeth and crusher parts, becomes brittle if it is heated and cooled slowly, so the heat from welding can easily crack it. It is often non-magnetic, which helps to identify it.

    An ordinary hardfacing deposit is usually not the right choice. Manganese steel is normally rebuilt with a matching austenitic manganese electrode, kept as cool as possible with short runs and no preheating beyond taking the chill off the part. The work-hardened surface that has formed in service should be ground off first. Always check the maker's guidance for the exact steel and electrode.

    Does the part need preheating before hardfacing?icon-minus-redicon-plus-red

    It depends on the base metal. Higher-carbon and low-alloy steels usually need preheating, and sometimes slow cooling afterwards, to stop the heat-affected zone cracking. Thicker parts need more heat than thin ones. Austenitic manganese steel is the exception: it should not be preheated beyond taking off the chill, and it needs to stay cool during welding.

    The temperature depends on the steel, its thickness and the electrode, so use the electrode data sheet and the welding procedure for the job rather than a rule of thumb. Let the part cool slowly in still air and do not quench it.