    OK Tigrod 13.08 is a 1.5Mn-0.4Mo-alloyed (ER80S-D2), copper-coated rod for the GTAW of creep-resistant steels of the same type, such as pipes in pressure vessels and boilers with a working temperature of up to about 500°C.  The rod can also be used for welding low-alloyed, high-tensile strength steels.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig Er80S-D2 FAQs

    Straight answers to the questions people ask most when choosing and using ER80S-D2 manganese-molybdenum TIG wire.

    What do the 80, S and D2 in the name mean?icon-minus-redicon-plus-red

    In the AWS A5.28 classification, ER means the product can be used as an electrode or a rod, 80 refers to the tensile strength class of the weld metal (about 80 ksi, or 550 MPa, minimum), S means a solid wire, and D2 identifies the manganese-molybdenum chemistry.

    The standard sets limits for carbon, manganese, silicon, molybdenum and other elements, and the maker's certificate shows the actual figures for the batch you receive. Manganese and molybdenum are added for strength, so check the certificate if your procedure calls for a particular chemistry.

    Which shielding gas and polarity should I use?icon-minus-redicon-plus-red

    Pure argon is the standard shielding gas for TIG welding of steel, and helium or helium-argon mixtures are used where a hotter arc is wanted. The electrode is normally connected negative on DC, because most of the arc heat goes to the work side and the tungsten stays cooler.

    The wire maker's data sheet gives the gas and current settings for the rod you have, so read it before you start. Set the gas flow so the pool is covered without turbulence, and shield the weld from draughts.

    Can I add hydrogen to the argon when welding with this wire?icon-minus-redicon-plus-red

    It is best not to. Argon with a few percent of hydrogen gives a cleaner-looking weld and faster travel, but it carries a risk of hydrogen cracking in carbon steels. Higher alloy and higher strength steels are more prone to hydrogen cracking, and in low alloy steels the cracks often appear in the weld metal itself.

    Use pure argon unless your qualified welding procedure specifically says otherwise, and keep the joint and rod clean and dry.

    Do I need preheat or post-weld heat treatment?icon-minus-redicon-plus-red

    Often, but it depends on the steel, the thickness and the code. Preheat slows cooling and lets hydrogen escape. The risk rises with carbon and alloy content and with section thickness, and a post-weld heat treatment may be needed to reduce hydrogen in the weld region.

    Maker guidance for related molybdenum steels shows the minimum preheat rising with thickness, a maximum interpass temperature, and a set soak time for stress relief. The correct figures for your job come from the qualified welding procedure, not from a general rule.