    Bohler CM 5-IG Steel TIG Wire, 1000mm Cut Length - AWS A5.28 ER80S-B6. 5Kg Pack
    BOHLER-TER80S-B6

    Select Option 
    Prices From £299.25 ex VAT

    GMAW wire is suitable for 5% Cr 0.5% Mo alloyed steels and steels for hot hydrogen service, particularly in oil refineries. Preferably used for steel grades such as X12CrMo5 and P5 at service temperatures up to +650°c.  The wire shows very good feeding characteristics, resulting in smooth welding and flow behaviour. Uniform copper bonding with low total copper content.  

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig Er80S-B6 FAQs

    Practical answers on choosing and using 5Cr-0.5Mo ER80S-B6 TIG wire for creep-resistant chrome-moly steels.

    What is ER80S-B6 TIG wire and what steels is it for?icon-minus-redicon-plus-red

    ER80S-B6 is a solid low alloy TIG filler containing roughly 5 per cent chromium and half a per cent molybdenum. It is chosen to match 5Cr-0.5Mo creep-resistant steels, which are used in pipework, tubes and vessels that run hot, for example in refineries and process plants.

    Matching filler metals exist for most creep-resistant steels. Check the parent steel specification, the drawing and your welding procedure to make sure this rod is the one called for.

    Why does 5Cr-0.5Mo steel need preheat before TIG welding?icon-minus-redicon-plus-red

    This steel hardens easily and forms hard, brittle martensite even when it cools slowly, so it is prone to cracking if welded cold. Preheat is essential for most creep-resistant steels, with a minimum in the region of 200 degrees C typical for 5Cr-0.5Mo, and the usual carbon equivalent method is not valid for these steels.

    The temperature you actually use must come from your qualified welding procedure and the governing code, not from a general figure.

    Do I need to back purge when TIG welding with this wire?icon-minus-redicon-plus-red

    In most pipe and tube work, yes. Higher-chromium alloys like this need an argon purge inside the bore when TIG welding the root, otherwise the inside of the root bead oxidises and becomes porous and rough, sometimes described as sugaring or coking.

    The purge gas should be pure argon and the flow and purge time are set by your procedure. Seal the ends of the pipe and keep the purge in place until enough weld has been laid to stop air getting in.

    Which shielding gas and polarity suit ER80S-B6?icon-minus-redicon-plus-red

    Like other TIG wires of this type, it is normally welded on DC electrode negative (DC-) with a pure argon shield. Shielding gas for these steels should be high purity and dry, because hydrogen from moisture contributes to cracking.

    Use good quality gas, hoses that are in good condition and tight fittings, and a suitable tungsten. Check the data sheet for the rod and the equipment manual for current settings, and use the values in your welding procedure.