WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : CM2IG  

    Bohler CM 2-IG Steel TIG Wire, 1000mm Cut Lengths - AWS A5.28 ER90S-B3. 5Kg Pack
    CM2IG

    Select Option 
    Prices From £151.20 ex VAT

    GMAW for 2.25% Cr 1% Mo alloyed boiler, plate and tube steels as well as in oil refineries e.g. in crack plants. Preferably used for the base metal 10CrMo9-10 (ASTM A335 Gr. P22). Approved in long-term condition up to +600°c service temperature. Also for similar alloyed quenched and tempered steels and case hardening steels. The deposit is noted for its good mechanical properties and cracking resistance, but also for its creep rupture strength which is within the scatter band of 10CrMo9-10. The wire shows very good feeding characteristics, resulting in smooth welding and wetting behaviour. 

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig Er90S-B3 FAQs

    Straight answers to the questions people ask most when choosing and using 2.25Cr-1Mo chromium-molybdenum TIG filler wire.

    What is ER90S-B3 TIG wire used for?icon-minus-redicon-plus-red

    ER90S-B3 is a low-alloy chromium-molybdenum solid rod, classed under the American standard for low-alloy steel filler rods. It contains roughly 2.25% chromium and 1% molybdenum, and it is used to weld creep-resistant steels of the same type, such as P22 pipe and 2.25Cr-1Mo plate used in power plant, refinery pipework and pressure vessels.

    The chromium and molybdenum help the weld keep its strength at high service temperatures. It is not a general-purpose steel rod, so use it where the drawing, code or welding procedure calls for a matching 2.25Cr-1Mo filler.

    Which base metals does it match, and what about dissimilar joints?icon-minus-redicon-plus-red

    It is chosen to match 2.25Cr-1Mo steels, for example P22 pipe and the equivalent plate grades. Other creep-resistant steels have their own matching fillers, so do not assume one rod fits them all.

    For dissimilar joints, the filler normally matches the less highly alloyed of the two steels, but the final choice should come from your qualified welding procedure and the applicable code. If you are unsure, check with your welding engineer before buying.

    How does ER90S-B3 differ from ER80S-B2 and ER90S-B9?icon-minus-redicon-plus-red

    The difference is mainly the chromium and molybdenum content, which sets the base metal each one matches. ER80S-B2 is a lower-alloy wire (about 1.25% chromium, 0.5% molybdenum) for steels such as P11. ER90S-B3 steps up to about 2.25% chromium and 1% molybdenum for P22. ER90S-B9 is in a different class altogether, with about 9% chromium, for P91-type steels.

    They are not interchangeable. Using a lower-alloy filler on P22, or the reverse, is generally not accepted on code work without engineering approval.

    Why do data sheets for this wire quote an X factor or low impurity levels?icon-minus-redicon-plus-red

    In 2.25Cr-1Mo weld metal, trace impurities such as phosphorus, tin, antimony and arsenic can gather at grain boundaries during long periods in the 400 to 600 degrees C range. This is called temper embrittlement, and it makes the weld less tough. The X factor is a calculation from these impurities, and a lower figure means lower risk.

    A low-impurity wire with a stated X factor limit is therefore chosen for pressure equipment that will run hot for years. If your specification sets a limit, check the wire's certificate to confirm it meets it.

    Shop Similar Categories