WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
  • Gullco-350  Gullco Stackable Oven with Thermostat. Temperature 100-550°F (38-288°C) 159Kg Capacity
  • Gullco-350  Gullco Stackable Oven with Thermostat. Temperature 100-550°F (38-288°C) 159Kg Capacity
Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

Rapid Ref : Gullco-350  

Gullco Stackable Oven with Thermostat. Temperature 100-550°F (38-288°C) 159Kg Capacity
Gullco-350

Select Option 
Prices From £1171.00 ex VAT

Features

  • Compact, modular design with control recessed for protection
  • Shelves easily removed to accommodate large sized loads
  • Oven fully insulated to prevent heat loss, pilot light indicates oven operation
  • Thermostat control, incorporating on/off switch, maintains oven temperature in 37.8 - 287.8°c range
  • Nesting Feet and Sockets for safe easy stacking

Product Details

Capacity: 159Kg
Outer Dimensions: 559mm x 559mm x 622mm
Inner Dimensions: 356mm x 405mm x 482mm
Unit Weight: 50Kg
Electrode Size: Up to 457mm

Brochures & Manuals

Stationary Ovens FAQs

Practical answers on using a floor-standing or stackable electrode oven to keep low-hydrogen welding rods dry.

Why do low-hydrogen electrodes need to be kept in a heated oven at all?icon-minus-redicon-plus-red

Low-hydrogen (basic) electrodes pick up moisture from the air quickly once they are exposed. Moisture in the coating is a source of hydrogen in the weld, and hydrogen is one of the three things that together cause hydrogen cracking, along with a hard, brittle structure and tensile stress. The cracks can appear many hours after welding has finished.

To keep weld hydrogen low, the electrodes must go into the weld dry. That means taking them straight from a sealed pack, or baking them and then storing them warm. A stationary oven does the storing job for a workshop or fabrication bay. Always follow the electrode maker's instructions and your welding procedure.

Can I use electrodes straight from a sealed pack, or do they always need the oven?icon-minus-redicon-plus-red

Electrodes in an undamaged, hermetically sealed pack can be used without baking. TWI notes that rods from vacuum packs can be used for a limited time after opening before enough moisture is absorbed to need baking, and gives up to 12 hours as one example. In hot, humid conditions the safe time can be shorter than the maker claims.

Once that time is up, or if a pack is torn or has lost its seal, the rods should go into the oven or be re-dried to the maker's instructions. Where your welding procedure or code sets its own exposure limit, that takes priority over general advice.

Should cellulosic electrodes be dried in the oven?icon-minus-redicon-plus-red

No, not in the way low-hydrogen types are. Cellulosic electrodes rely on some moisture in the coating to work properly, and TWI advises that they should not be dried and should be used directly from the manufacturer's packaging. If rods get soaked, they are best discarded rather than dried.

One oven maker's re-drying chart also lists cellulosic types as not recommended for re-drying. The electrode maker's data sheet says how each type should be stored. Keep cellulosic rods separate from low-hydrogen rods so the two are never mixed up or put through a low-hydrogen drying cycle.

Should electrodes be left in their packets when I put them in the oven?icon-minus-redicon-plus-red

No. One stationary oven maker's manual states that electrodes must always be removed from their wrappers or packets before heating. Leaving them wrapped increases the risk of fire, and the moisture is not carried away and can be reabsorbed by the coating when the rods cool.

Take the rods out, place them in the trays or racks provided, and dispose of the packaging. The same manual notes that all mineral-coated electrodes begin absorbing moisture once unpacked, and that damp rods lead to more spatter, undercut, poor slag removal and porosity. Follow the maker's manual for your oven.