WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : TIG625  

    INCONEL Filler Metal 625 High Nickel TIG Wire, 1000mm Cut Lengths - AWS A5.14 ERNiCrMo-3, 4.54Kg Pack
    TIG625

    Select Option 
    Prices From £503.40 ex VAT

     

    INCONEL Filler Metal 625 is used for gas-metal-arc and gas-tungsten-arc welding of INCONEL alloy 625, INCOLOY alloy 825, INCOLOY alloy 25-6MO, and a range of high alloy austenitic and super austenitic stainless steels. It is also used for surfacing of steel, for welding 9% Ni steels, and for welding various corrosion-resistant alloys such as alloy 20. INCONEL Filler Metal 625 can be used for joining and overlaying with INCOFLUX NTl00 Submerged Arc Flux. The weld metal has high strength over a broad temperature range and has resistance to localized attack such as pitting and crevice corrosion.

    INCONEL Filler Metal 625 is useful for many dissimilar joints involving INCONEL and INCOLOY alloys, carbon steels, low-alloy steels, and stainless steels.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure
       Lloyds Certificate (ISO9001-AS9120)

    High Nickel TIG Wire FAQs

    Straight answers to the questions people ask most when choosing and using nickel alloy TIG filler wire.

    Why does cleanliness matter so much with nickel alloys?icon-minus-redicon-plus-red

    Nickel alloys are easily embrittled at high temperature by sulphur, lead, phosphorus, boron and bismuth. These can come from oils, grease, cutting fluids, paints, marker pens and temperature-indicating crayons. Contamination of this kind can cause cracking in the weld or heat-affected zone.

    Keep the joint, the filler wire and your tools free of these materials, and use brushes and tools kept only for nickel alloys. Avoid marking with ordinary markers or crayons near the weld.

    Which shielding gas should I use for TIG welding nickel alloys?icon-minus-redicon-plus-red

    Pure argon is the usual choice, and argon with helium or with a small addition of hydrogen is also used for some alloys. A hydrogen addition can improve the fluidity of the weld pool and give cleaner welds, but it is not suitable for every alloy, so check the filler maker's recommendation.

    Good gas coverage matters, because oxygen and nitrogen from the air cause porosity. Keep gas hoses in good condition, avoid draughts, and use a back purge where the root side of the joint needs protecting.

    What is the best technique for welding nickel alloys?icon-minus-redicon-plus-red

    Nickel alloys do not flow like mild steel, so the weld does not wet out sideways much. Use stringer beads with little weaving, keep the heat input modest and aim for a slightly convex bead profile. Heat input and interpass temperature limits depend on the alloy, so follow the filler maker's guidance.

    Grind out the start and stop points of each run to avoid porosity. Higher current does not usually give deeper penetration, and a joint preparation with a wide enough angle helps you reach the root.

    Why does a nickel filler get used to join stainless steel to carbon steel?icon-minus-redicon-plus-red

    Nickel alloy fillers generally perform well in dissimilar joints between ferritic and austenitic steels. The thermal expansion of nickel alloys sits between that of ferritic steel and austenitic stainless steel, so the joint suffers less thermal fatigue when it heats and cools repeatedly.

    The right nickel filler for a dissimilar joint depends on the metals and the service conditions, such as temperature and corrosion. Check the filler maker's data sheet and, for critical work, the specification you are working to.