Straight answers to the questions people ask most when choosing, storing and using flux-coated aluminium electrodes for manual metal arc welding.
What are aluminium MMA electrodes used for?

They are flux-coated aluminium alloy rods for welding and repairing aluminium with a standard stick (MMA) welding set, without needing a gas bottle. Typical classes are the aluminium-silicon types, such as 4043 (AlSi5) for general-purpose work on common aluminium alloys, and 4047 (AlSi12) where a more fluid, higher-silicon filler is wanted. Pure aluminium types also exist for commercially pure aluminium.
They are most useful for site and workshop repairs and fabrication in thicker sections, where TIG or MIG equipment is not to hand. Check the class on the pack against the alloy you are joining.
Which polarity do aluminium electrodes need?

Aluminium stick electrodes are normally run on DC with the electrode connected to the positive terminal (often called DC electrode positive or reverse polarity). They are not usually suitable for AC.
The electrode box or data sheet states the polarity and the current range for each diameter, so follow that. If your machine is AC-only, it will not normally run these electrodes, and TIG or MIG may be a better route for aluminium.
Can I use a 4043-type electrode on any aluminium alloy?

No. Silicon-bearing 4043-type filler is a general-purpose choice for many alloys, but it is not recommended on high-magnesium 5xxx alloys. Welding those with it can give a brittle weld, and a magnesium-bearing 5xxx filler is normally used instead. Makers usually put the dividing line at around 2.5 per cent magnesium, but a few alloys sit close to the line, so check with the filler maker or the welding specification.
The weld colour after anodising will also not match the parent metal. Identify the parent alloy before choosing the electrode class.
How should I store aluminium electrodes?

The flux coating is strongly hygroscopic, meaning it soaks up moisture from the air. Makers advise storing the electrodes in an absolutely dry place and re-drying them if necessary before use.
Keep them in their sealed pack until needed, put any unused electrodes back in a dry container, and do not leave them in a cold van or damp store. Damp coating can cause spatter, an unstable arc and porosity in the weld. The drying temperature and time depend on the maker, so follow the pack or data sheet.
How do I prepare aluminium before welding with a stick electrode?

Degrease the joint and the surrounding area first with a suitable solvent and a clean cloth, then remove the oxide layer mechanically with a stainless steel brush kept only for aluminium. Use light pressure, because heavy brushing can smear the oxide into the surface.
Weld soon after cleaning, as the oxide layer re-forms and can pick up moisture. Keep aluminium work away from steel grinding dust and tools, which cause contamination. Dirty or damp surfaces are a leading cause of porosity.
Do I need to remove the slag after welding aluminium?

Yes, and completely. The flux residue left on and beside the bead is corrosive, and it can attack the aluminium if it stays in place, especially in damp conditions or in crevices.
Chip and brush off the residue as soon as the weld has cooled enough to handle. Makers may also specify a further cleaning step for their electrodes, such as washing, so follow their instructions. Any chemical cleaning must be carried out only under suitable health and safety controls.
Do I need to preheat aluminium before stick welding?

It depends on the thickness, the alloy and the surroundings. Aluminium conducts heat away quickly, so thick sections often benefit from preheating to help the weld pool fuse and to reduce the current needed. Thin material usually needs none.
Preheat is no substitute for good cleaning, because dirt and moisture still cause porosity. Use the temperature in the electrode maker's instructions or your welding procedure, and do not overheat the work, which can affect the strength of some alloys.