The website is working fine. Please feel free to place orders. WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : 1196X  

    Bohler FOX CEL Cellulosic Electrodes. E6010
    1196X

    Select Option 
    Prices From £57.72 ex VAT

    Cellulose electrode for vertical-down welding of large diameter pipelines; suitable for root runs (vertical down and vertical up), hot passes, filler and cover layers. Especially recommended for root run welding. Highly economical compared with vertical-up welding. Apart from its excellent welding and gap bridging characteristics, FOX CEL offers a weld deposit with outstanding impact strength values and thus offers the benefit of still more safety in the field welding of pipelines. BÖHLER FOX CEL can be used in sour gas applications (HIC-Test acc. NACE TM-02-84).

    Classifications

    EN ISO 2560-A - E 38 3 C 2 1

    EN ISO 2560-B - E 43 10 A U

    AWS A5.1 - E6010

    AWS A5.1M - E4310

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Cellulosic Pipe Electrodes FAQs

    Straight answers to common questions about cellulosic E6010 and E6011 electrodes used for pipe root runs and vertical-down welding.

    What is vertical-down or stovepipe welding and why is the root run so important?icon-minus-redicon-plus-red

    Stovepipe welding is manual metal arc welding run downwards on a pipe, from the top towards the bottom, using a cellulosic electrode. It is much faster than welding uphill, which is why it is used for laying long pipelines.

    The root run is the most critical because the quality of the whole joint depends on it, and it also limits how fast joints can be completed. The root and the following hot pass need a welder with the right skill and a qualified procedure.

    Do I need to dry cellulosic electrodes?icon-minus-redicon-plus-red

    No. Unlike low hydrogen electrodes, cellulosic electrodes rely on the moisture and hydrogen in the coating for their gas shield, so they should be used straight from their sealed packaging and not baked in an oven. Over-drying can spoil how they run.

    Store them in unopened packaging in a dry place and keep opened cans closed. If electrodes have become damp or soaked, follow the maker's instructions on what to do, and discard any that are badly affected. Damp coatings can cause poor arc behaviour and porosity.

    Why is there a risk of hydrogen cracking with cellulosic electrodes?icon-minus-redicon-plus-red

    The gas shield from the coating contains hydrogen, so the weld metal and the heat-affected zone pick up a high level of diffusible hydrogen. In susceptible steels this can lead to cold cracking, which may appear some time after welding.

    The usual precautions are to follow the welding procedure for preheat where it is needed, to deposit the hot pass promptly after the root, and to use steel with good resistance to cracking. Avoid using cellulosic electrodes for single-pass fillet welds. The procedure should be set by a competent person, not by guesswork.

    Which polarity and welding current should I use?icon-minus-redicon-plus-red

    E6010 electrodes run on direct current with the electrode positive, and E6011 can also be used on alternating current. Cellulosic electrodes are normally run at higher currents than rutile electrodes, but the current is limited in practice by spatter.

    The right current depends on the electrode diameter, the position and the joint, so use the range printed on the packaging or data sheet and adjust to suit the root gap and the pool. A constant-current set is recommended because it helps offset the natural movement of the hand.

    Shop Similar Categories