Bohler Low Hydrogen FAQs
Straight answers to the questions people ask most when choosing and using low hydrogen stick electrodes for mild, higher strength and chrome-moly steels.
Do chrome-moly low hydrogen electrodes need preheat and heat treatment after welding?

Usually, yes. Alloyed and higher-carbon steels are more prone to hydrogen cracking, so they normally need low hydrogen consumables together with preheat, controlled cooling and often a post-weld heat treatment. How much depends on the steel grade, thickness, restraint and heat input.
The temperatures and times should come from the welding procedure, the governing code and the electrode maker's data sheet, not from a rule of thumb. If your procedure calls for post-weld heating or heat treatment, do not skip it to save time.
How low does the hydrogen level need to be for thick or high strength steel?

The lower the diffusible hydrogen, the lower the cracking risk, and the requirement gets tighter as the steel gets stronger, thicker or more restrained. For many ordinary jobs a low hydrogen basic electrode is enough, but for high restraint, heavy sections or alloyed weld metal, stricter hydrogen limits and preheat may be required.
Hydrogen levels are graded in standard scales running from high to ultra-low, and a lower marking such as H4 means a tighter limit than H8. Your procedure should say what grade is needed; choose an electrode marked to meet it.
What does the classification on a low hydrogen electrode box tell me?

In a code such as E7018, the E means a covered stick electrode, and the first digits give the minimum tensile strength of the weld metal in a standard unit, so 70 means a 70 class strength. The next digit indicates which positions it can be used in, and the last two digits together tell you the coating type and the current it runs on.
A suffix such as -1, a hydrogen figure or a letter and number for alloy content shows added toughness, a hydrogen limit or the alloy type. Use the box, the data sheet and your procedure to confirm that the electrode matches the job.
What is an E8018-B2 type electrode used for?

This type is a low hydrogen electrode with chromium and molybdenum in the deposit, designed to match 1.25Cr-0.5Mo creep-resistant steels such as those used in pipework and pressure parts running at raised temperatures. The alloy gives the weld strength and resistance to creep and oxidation at heat.
Because the weld metal is alloyed, it is more sensitive to hydrogen cracking than plain mild steel, so careful storage, preheat and usually post-weld heat treatment apply. Always use the electrode named in the welding procedure, and check the maker's data sheet for the exact temperatures and conditions.