Shielding gas is leaking or my welds are porous. Which torch parts should I check first?icon-minus-redicon-plus-red

Porosity in TIG welding is most likely caused by contamination or loss of gas shielding, and common causes include leaks in the gas line, too high a gas flow rate and draughts. A torch maker's troubleshooting guide adds a defective gas hose or loose connection, and a blockage or leak in the hoses or torch.

So check the gas hose and every joint, the back cap and its O-ring, the O-rings behind the collet body or gas lens, and the cup for cracks. Replace worn O-rings and damaged cups rather than tightening them harder, remove draughts, and keep the metal and filler clean.

How far can I let the tungsten stick out of the cup?icon-minus-redicon-plus-red

Keep it as short as the joint allows. A torch maker's technical guide lists excessive electrode stick-out as a cause of inadequate shielding and of tungsten inclusions in the weld, and recommends reducing it, using a larger cup or changing to gas saver or gas lens parts.

A gas lens gives a smoother gas stream, so a longer stick-out is practical, which helps in corners. A common rule of thumb is a stick-out of about the cup's inside diameter, but treat it as a starting point, because cup size, gas flow, torch angle and draughts all matter. If you see discoloured welds or porosity, shorten the stick-out or recheck the gas.

Why do my cups keep cracking, and how can I make them last longer?icon-minus-redicon-plus-red

A torch maker's guide to short parts life lists cups shattering or cracking in use, and suggests changing the cup size or type and the tungsten position. The same guide says not to run a torch beyond its rated capacity, which protects the torch head. Knocks, dropping the torch and over-tightening the cup also crack cups, and glass and ceramic are both brittle.

To make cups last, choose a cup suited to the job and current, avoid touching it against hot work, screw it on firmly by hand only, and let the torch cool before cleaning. Replace a chipped or cracked cup, because damage disturbs the gas flow.

What safety points apply to grinding and handling tungsten electrodes?icon-minus-redicon-plus-red

Some tungsten electrodes contain thoria, and grinding creates the greatest hazard because it releases fine, potentially radioactive dust that can be inhaled. Use a dedicated grindstone with local dust extraction that collects the dust in a sealed bag, a simple filter mask unless very few electrodes are used, and eye protection if the grinder has no screen.

Ceriated or lanthanated electrodes are acceptable alternatives for DC, and zirconiated is preferred for AC, with little radioactivity. Follow the electrode maker's instructions and your risk assessment.

How much gas flow should I use with a gas lens or a larger cup?icon-minus-redicon-plus-red

Too high a gas flow rate is a common cause of porosity, and a torch maker's guide warns against raising the flow beyond the point where it creates excessive turbulence. Too much flow can pull air into the weld zone, while too little leaves it unprotected.

There is no single correct figure, because the right setting depends on the cup size, the joint, the stick-out, draughts and the metal. Start from the torch manual or your welding procedure, and adjust by watching for discolouration or pinholes. A gas lens gives a smoother flow, and some users find they can reduce the flow slightly, but check this for your own setup rather than assuming it.

What is a large-diameter gas lens set and when would I use one?icon-minus-redicon-plus-red

A large-diameter set uses a wider gas lens with a bigger cup, so the shield of gas covers a larger area around the arc. A gas lens is fitted to give smooth, laminar gas flow for sensitive operations such as corner and edge joints, and nozzle choice depends mainly on electrode diameter and access. More reactive metals need better coverage than a plain cup gives.

The lens, insulator and cup normally have to be used together, so you cannot usually mix them with standard-size parts. The bigger cup is bulkier, which can limit access in tight joints. Check the set suits your torch and tungsten diameter.

CK3 Series Parts Breakdown