Ceramic Backing Tiles

Click on product to get full infomation sheet on all tiles

Ceramic Backing Tiles FAQs

Straight answers to the questions people ask most when choosing and using ceramic weld backing tiles.

What are ceramic backing tiles and what are they used for?icon-minus-redicon-plus-red

Ceramic backing tiles are strips of heat-resistant ceramic, usually fixed along the back of a joint with an adhesive aluminium foil tape. They support the molten weld metal from behind, so you can make a full-penetration weld from one side only.

They are widely used in shipbuilding, structural steelwork, tanks and pressure parts where the back of the joint cannot be reached, or where welding and then gouging from the second side would take too long. They are used with MIG, flux-cored, stick and submerged arc welding, depending on the type of tile.

Why use ceramic backing instead of a steel backing strip or welding from both sides?icon-minus-redicon-plus-red

A steel backing strip stays in the joint, which can create a crevice, add weight and sometimes cause problems with fatigue or corrosion, and it must be the right material. Welding from both sides means turning the work, back gouging or grinding the root, and welding again.

Ceramic tiles are removed afterwards, leaving a clean, smooth root without the extra steps or a permanent strip. Whether ceramic backing is allowed for a job is set by the welding procedure, so check what your specification permits.

How do I choose the right tile shape and size?icon-minus-redicon-plus-red

The tile shape controls the profile of the root bead, and it must suit the joint. Flat tiles, grooved tiles with a round or square channel, and tiles with different groove widths are made for different joint preparations, root gaps and plate thicknesses. Some are designed for corner or fillet joints, and others for curved surfaces.

The tile maker's guidance links each tile to the root gap and bevel it was designed for, so match the tile to your joint preparation and welding procedure. If you are unsure, ask the maker or our team.

How are ceramic tiles fixed to the work?icon-minus-redicon-plus-red

Most tiles come mounted on a strip of foil tape with an adhesive backing. The tape is pressed onto the back of the joint so the tile sits centred under the root gap, and the foil is smoothed down along its length so it makes good contact.

Follow the instructions supplied with the tiles for preparing the surface and for the temperature range in which the adhesive works. In general, the metal should be clean and free of moisture, oil and loose material. Make sure the tiles butt neatly end to end so there is no gap between them.

Which welding processes and positions can I use with ceramic backing?icon-minus-redicon-plus-red

Ceramic backing is used with several arc welding processes, and tiles are made for particular processes, current levels and positions. Check the tile's specification and your welding procedure to confirm that the type suits your process and position.

Ceramic backing supports the molten metal from behind. Do not assume it also protects the root from the air. For metals that oxidise easily on the underside, check your procedure and the material's requirements for whether extra root protection is needed.

Why is my root bead poor or not fusing at the edges?icon-minus-redicon-plus-red

The usual causes are a root gap that is too narrow or wide for the tile, a tile that does not sit squarely under the joint, poor contact between the tile and the metal, or settings and technique that don't suit the joint. Lack of fusion at the edges can come from too low a current or travel that is too fast.

Welding over damp tiles can cause porosity. Check the fit-up, the tile position and the foil seal, and prove the settings on a test piece before welding the real joint.