Tig Er70S-6 FAQs
Answers to common questions about ER70S-6 mild steel TIG filler rod: what it is, how to choose it, use it and look after it.
What is ER70S-6 TIG filler rod and what is it used for?

ER70S-6 is a solid steel filler rod for TIG welding mild and medium tensile carbon-manganese steels. Maker data sheets show a high manganese content (about 1.4 to 1.85%) and a high silicon content (about 0.8 to 1.15%). These act as deoxidisers, helping to produce a clean, sound weld metal.
It is widely used for general fabrication, repair and structural work. Check the drawing or welding procedure first, since the specification may name a particular filler.
What do the letters and numbers in ER70S-6 mean?

This is an American classification. The R means it can be used as a rod, the 70 refers to the minimum tensile strength of the weld metal in thousands of pounds per square inch (70 ksi, about 480 MPa), and the S shows it is a solid wire rather than a flux-cored one. The final 6 identifies the chemical composition group.
Different makers market it under their own names, but the classification tells you the rod meets the same composition and strength requirements. Check the certificate or packaging for the classification before use.
What shielding gas and polarity should I use with ER70S-6 for TIG?

Maker data sheets for TIG rod of this class give pure argon shielding and DC electrode negative (DCEN, also called straight polarity). This is different from MIG welding with the same classification, where an argon-CO2 mixture or CO2 is used with electrode positive.
Set gas flow and current for the joint, cup size and torch, and follow the rod maker's data sheet. Too much flow can cause turbulence and draw air into the gas shield, which can cause porosity, so more is not always better.
What diameter of ER70S-6 rod should I choose?

A common choice for mild steel is 1.6 mm rod for thinner material and general fabrication, and 2.4 mm rod for thicker sections or larger weld profiles. Treat that as a starting point, because the exact rule varies.
A rod that is too thin for the job melts too fast in a hot puddle, while a very large rod on low current can chill the pool and give an uneven bead. Try the size on offcuts of the same steel, and check your welding procedure, which may fix the diameter.