    ESAB OK 48.00 Low Hydrogen Electrodes, E7018 H4 R
    48002530KX

    Select Option 
    Prices From £14.84 ex VAT

    A reliable, general-purpose LMA electrode for mild and low-alloy steels. ESAB OK 48.00 deposits a tough, crack-resistant weld metal. High welding speed in the vertical-up position. ESAB OK 48.00 is insensitive to the composition of the base material within fairly wide limits. The electrode can be used for welding structures where difficult stress conditions cannot be avoided.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    ESAB Low Hydrogen FAQs

    Straight answers to the questions people ask most when choosing, storing and using low hydrogen (basic) stick electrodes.

    What do the letters and numbers in a class such as E7018 H4 R mean?icon-minus-redicon-plus-red

    In the American system, E means a covered electrode, 70 relates to the minimum tensile strength of the weld metal, and the last two digits describe the coating, the positions it can be used in and the current type. The 18 identifies an iron powder, basic low hydrogen coating.

    H4 is a diffusible hydrogen designator, meaning the weld metal is limited to a maximum of 4 ml of hydrogen per 100 g under the test conditions. R shows the coating has met a low moisture pickup test. The data sheet states the full classification, so check it matches your procedure.

    What should I do with electrodes that have been left out in the open?icon-minus-redicon-plus-red

    Do not just weld with them. Moisture picked up by the coating puts hydrogen back into the weld, which can cause porosity and cracking, especially in higher strength steels. A holding oven keeps dry electrodes dry; it does not dry out damp ones.

    Electrodes that have been exposed for longer than the maker allows normally need re-baking at the temperature and for the time the maker specifies, in a proper baking oven with the rods spread out. Over-baking or repeated re-baking can make the coating flake, and electrodes with a damaged coating should be thrown away. Check the data sheet for the limits.

    What current and polarity should I use?icon-minus-redicon-plus-red

    Most low hydrogen electrodes are designed for DC with the electrode positive (DCEP), which gives the most stable arc and the best control. Some types will also run on AC from a suitable machine, but the arc is usually less steady and the machine needs enough open circuit voltage.

    The data sheet lists the polarity and the current range for each diameter, so set the current within that range rather than guessing. Using the wrong polarity can give an unstable arc, extra spatter and porosity.

    How should I strike the arc and hold the arc length?icon-minus-redicon-plus-red

    Keep the arc very short. Some makers' data sheets give a figure of less than half the rod diameter. These electrodes are unforgiving of a long arc, because it weakens the gas shield and lets air into the weld pool, which is a common cause of porosity.

    Strike the arc just ahead of where the weld will start, then move back and begin welding once the rod tip is hot, which reduces start porosity. Hold the rod at a slight drag angle for flat and horizontal work, and use a small weave or a slight upward push for vertical-up. Follow the data sheet for the current range and technique.