Ceramic Backing Tiles FAQs
Straight answers to the questions people ask most when choosing and using ceramic weld backing tiles.
What are ceramic backing tiles and what are they used for?

Ceramic backing tiles are strips of heat-resistant ceramic, usually fixed along the back of a joint with an adhesive aluminium foil tape. They support the molten weld metal from behind, so you can make a full-penetration weld from one side only.
They are widely used in shipbuilding, structural steelwork, tanks and pressure parts where the back of the joint cannot be reached, or where welding and then gouging from the second side would take too long. They are used with MIG, flux-cored, stick and submerged arc welding, depending on the type of tile.
Why use ceramic backing instead of a steel backing strip or welding from both sides?

A steel backing strip stays in the joint, which can create a crevice, add weight and sometimes cause problems with fatigue or corrosion, and it must be the right material. Welding from both sides means turning the work, back gouging or grinding the root, and welding again.
Ceramic tiles are removed afterwards, leaving a clean, smooth root without the extra steps or a permanent strip. Whether ceramic backing is allowed for a job is set by the welding procedure, so check what your specification permits.
How are ceramic tiles fixed to the work?

Most tiles come mounted on a strip of foil tape with an adhesive backing. The tape is pressed onto the back of the joint so the tile sits centred under the root gap, and the foil is smoothed down along its length so it makes good contact.
Follow the instructions supplied with the tiles for preparing the surface and for the temperature range in which the adhesive works. In general, the metal should be clean and free of moisture, oil and loose material. Make sure the tiles butt neatly end to end so there is no gap between them.
Why is my root bead poor or not fusing at the edges?

The usual causes are a root gap that is too narrow or wide for the tile, a tile that does not sit squarely under the joint, poor contact between the tile and the metal, or settings and technique that don't suit the joint. Lack of fusion at the edges can come from too low a current or travel that is too fast.
Welding over damp tiles can cause porosity. Check the fit-up, the tile position and the foil seal, and prove the settings on a test piece before welding the real joint.