WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE

Hard Facing MIG Wire

Hard Facing MIG Wire FAQs

Straight answers to the questions buyers ask most when choosing and using hardfacing cored wire for wear-resistant overlays.

How do I choose the right hardfacing wire for my wear problem?icon-minus-redicon-plus-red

Start by working out how the part wears. Sliding of loose material under low pressure (low-stress abrasion) usually calls for a harder deposit with plenty of carbides. Crushing and grinding under high pressure needs a tougher deposit with well-spread carbides. Heavy pounding or gouging usually points to a work-hardening austenitic manganese type, and metal-to-metal wear or galling suits a tool-steel type of deposit.

Most real parts suffer a mix of wear types, so aim for the best balance rather than the hardest deposit. Check the base metal too, because it affects preheat and whether a buffer layer is needed. Our team can help you match a wire to the job.

What is the difference between chromium carbide, martensitic and manganese hardfacing wires?icon-minus-redicon-plus-red

Chromium carbide deposits are the usual choice for abrasion with low to moderate impact. They are very hard but brittle, so they tend to show fine cracks and are usually limited in how many layers can be built up.

Martensitic deposits are a compromise: good abrasion resistance with better toughness, so they suit mixed abrasion and impact, and they are often used as a build-up as well. Austenitic manganese deposits are tough and harden under hammering, so they suit heavy impact and rebuilding manganese steel parts, but they are not the best choice for pure sliding abrasion. Always check the maker's data sheet for the alloy you are considering.

Do I need a buffer layer before hardfacing?icon-minus-redicon-plus-red

Often, yes. A buffer or build-up layer gives the hard deposit a tough, crack-resistant base, and it is commonly used on steels that harden easily and when rebuilding worn parts. The buffer must be compatible with both the base metal and the final hardfacing alloy.

On manganese steel, an austenitic buffer is normally used rather than a carbon steel build-up. Before welding, remove the old work-hardened surface from manganese steel, because leaving it in place can cause cracking under the weld. If a wire's data sheet specifies a buffer layer for your base metal, follow it.

Do I need to preheat before hardfacing?icon-minus-redicon-plus-red

It depends on the base metal. Higher-carbon and low-alloy steels, tool steels, martensitic stainless steels and most cast irons are normally preheated, and the amount depends on the carbon and alloy content, the thickness and the wire. Preheating also helps reduce distortion and cracking, and slow cooling afterwards helps protect the heat-affected zone.

Austenitic manganese steel is different. It should not be preheated much and should not be allowed to get too hot, because excessive heat makes it brittle, so keep the base metal below the maximum temperature the maker gives. Always follow the wire maker's data sheet and your welding procedure.

Is it normal for a hardfacing deposit to crack?icon-minus-redicon-plus-red

With chromium carbide types, fine cracks running across the beads (check cracking) are usually normal. They form as the hard, brittle deposit cools and contracts, and they relieve stress. They are generally not harmful to wear performance unless the part sees a corrosive service.

Cracks that run along the bead, or that go down into the base metal (underbead cracking), are a warning sign. They can lead to the deposit breaking away. Common causes are too little dilution with the base metal, no buffer layer, too little preheat or cooling too quickly. If your deposit shows irregular cracking, review the procedure and the data sheet.

How many layers of hardfacing can I put on?icon-minus-redicon-plus-red

It depends on the alloy, the base metal and the process. The first layer is diluted most by the base metal, so its hardness is usually lower than the data sheet value, and two or three layers are often needed to reach the quoted hardness. Chromium carbide types are normally limited in the number of layers because of cracking, while manganese types can usually be built up further unless the maker says otherwise.

On high-carbon steels the number of layers is often limited because of cracking risk. Check the data sheet for the maximum layer count and overall thickness for the wire you are using.