Tig Er90S-B3 FAQs
Straight answers to the questions people ask most when choosing and using 2.25Cr-1Mo chromium-molybdenum TIG filler wire.
What is ER90S-B3 TIG wire used for?

ER90S-B3 is a low-alloy chromium-molybdenum solid rod, classed under the American standard for low-alloy steel filler rods. It contains roughly 2.25% chromium and 1% molybdenum, and it is used to weld creep-resistant steels of the same type, such as P22 pipe and 2.25Cr-1Mo plate used in power plant, refinery pipework and pressure vessels.
The chromium and molybdenum help the weld keep its strength at high service temperatures. It is not a general-purpose steel rod, so use it where the drawing, code or welding procedure calls for a matching 2.25Cr-1Mo filler.
How does ER90S-B3 differ from ER80S-B2 and ER90S-B9?

The difference is mainly the chromium and molybdenum content, which sets the base metal each one matches. ER80S-B2 is a lower-alloy wire (about 1.25% chromium, 0.5% molybdenum) for steels such as P11. ER90S-B3 steps up to about 2.25% chromium and 1% molybdenum for P22. ER90S-B9 is in a different class altogether, with about 9% chromium, for P91-type steels.
They are not interchangeable. Using a lower-alloy filler on P22, or the reverse, is generally not accepted on code work without engineering approval.
Does the weld need post-weld heat treatment?

Almost always. Post-weld heat treatment is mandatory in most application codes for creep-resistant steels. It softens the hard as-welded structure, improves toughness and sets up the carbide structure needed for long-term creep strength. The temperature and hold time come from the procedure and code, so do not take figures from a rod description.
Plan the heat treatment before you start welding, because it affects when the joint can be released and inspected.
Why do data sheets for this wire quote an X factor or low impurity levels?

In 2.25Cr-1Mo weld metal, trace impurities such as phosphorus, tin, antimony and arsenic can gather at grain boundaries during long periods in the 400 to 600 degrees C range. This is called temper embrittlement, and it makes the weld less tough. The X factor is a calculation from these impurities, and a lower figure means lower risk.
A low-impurity wire with a stated X factor limit is therefore chosen for pressure equipment that will run hot for years. If your specification sets a limit, check the wire's certificate to confirm it meets it.