TIG ER80S-B6

Description: 

5Cr-0.5Mo-alloyed (ER80S-B6), copper-coated rod for the GTAW of creep-resistant steels of similar composition. The rod is also suitable for welding high strength steels with a minimum yield strength of up to 730 MPa. AWS has changed the classification for this product. The previous classification was A5.9 ER50

Welding current: DC-
Wire composition, wt.%

  C Mn Si Ni Cr Mo
Typical 0.07 0.48 0.44 0.06 5.73 0.58

Tig Er80S-B6 FAQs

Practical answers on choosing and using 5Cr-0.5Mo ER80S-B6 TIG wire for creep-resistant chrome-moly steels.

What is ER80S-B6 TIG wire and what steels is it for?icon-minus-redicon-plus-red

ER80S-B6 is a solid low alloy TIG filler containing roughly 5 per cent chromium and half a per cent molybdenum. It is chosen to match 5Cr-0.5Mo creep-resistant steels, which are used in pipework, tubes and vessels that run hot, for example in refineries and process plants.

Matching filler metals exist for most creep-resistant steels. Check the parent steel specification, the drawing and your welding procedure to make sure this rod is the one called for.

Why does 5Cr-0.5Mo steel need preheat before TIG welding?icon-minus-redicon-plus-red

This steel hardens easily and forms hard, brittle martensite even when it cools slowly, so it is prone to cracking if welded cold. Preheat is essential for most creep-resistant steels, with a minimum in the region of 200 degrees C typical for 5Cr-0.5Mo, and the usual carbon equivalent method is not valid for these steels.

The temperature you actually use must come from your qualified welding procedure and the governing code, not from a general figure.

Is post-weld heat treatment needed after welding with ER80S-B6?icon-minus-redicon-plus-red

Usually yes. Post-weld heat treatment (PWHT) softens the hard structure left in the weld and heat affected zone, improves toughness and controls the size of the strengthening precipitates. It is normally required by the application codes for these steels, and a typical range for 5Cr-0.5Mo is roughly 710 to 750 degrees C.

Exact temperature, soak time and heating and cooling rates depend on the code, the thickness and your procedure.

What interpass temperature should I keep when TIG welding 5Cr-0.5Mo?icon-minus-redicon-plus-red

Interpass temperature is the highest temperature the joint is allowed to reach before the next run. A maximum of about 350 degrees C is typical for this steel, but the governing code and your welding procedure decide the figure you must work to.

Measure it with a contact thermometer or temperature crayons at the joint, and let it cool to the limit before the next pass. Keeping the joint above the preheat temperature between passes is just as important.

Do I need to back purge when TIG welding with this wire?icon-minus-redicon-plus-red

In most pipe and tube work, yes. Higher-chromium alloys like this need an argon purge inside the bore when TIG welding the root, otherwise the inside of the root bead oxidises and becomes porous and rough, sometimes described as sugaring or coking.

The purge gas should be pure argon and the flow and purge time are set by your procedure. Seal the ends of the pipe and keep the purge in place until enough weld has been laid to stop air getting in.

How does ER80S-B6 differ from the lower chrome-moly TIG wires?icon-minus-redicon-plus-red

The main difference is the chromium and molybdenum content, which suits the wire to a particular steel and its service temperature. ER80S-B6 is a 5 per cent chromium wire, while lower alloy wires carry less chromium and are matched to different steels with different preheat and heat treatment temperatures.

Do not substitute one for another because they look alike. Match the filler to the parent steel as the procedure states, and keep rods identified. If a joint connects two different alloy steels, the filler normally matches the lower alloy side, so follow the procedure for that joint.

Which shielding gas and polarity suit ER80S-B6?icon-minus-redicon-plus-red

Like other TIG wires of this type, it is normally welded on DC electrode negative (DC-) with a pure argon shield. Shielding gas for these steels should be high purity and dry, because hydrogen from moisture contributes to cracking.

Use good quality gas, hoses that are in good condition and tight fittings, and a suitable tungsten. Check the data sheet for the rod and the equipment manual for current settings, and use the values in your welding procedure.