TIG ER90S-B3

Description:

A copper coated, low-alloyed, chromium-molybdenum (2,5% Cr, 1,1 % Mo), solid wire for GMAW of creep resistant steels like SA-387 Grade 22, A335 Grade P22 or similar materials. High purity wire with a guaranteed Bruscato factor X<15. Preheat and interpass temperature 200-350 °C. Usually welding is followed by a stress relieving heat treatment at 600-700 °C

Welding current: DC-
Wire composition, wt.%

  C Si Mn P S Cr Mo Cu X
Min 0.07 0.40 0.40     2.30 0.90    
Typical 0.08 0.5 0.5 0.01 0.01 2.4 1.0 0.15
Max 0.12 0.70 0.70 0.025 0.015 2.70 1.20 0.35  15

Tig Er90S-B3 FAQs

Straight answers to the questions people ask most when choosing and using 2.25Cr-1Mo chromium-molybdenum TIG filler wire.

What is ER90S-B3 TIG wire used for?icon-minus-redicon-plus-red

ER90S-B3 is a low-alloy chromium-molybdenum solid rod, classed under the American standard for low-alloy steel filler rods. It contains roughly 2.25% chromium and 1% molybdenum, and it is used to weld creep-resistant steels of the same type, such as P22 pipe and 2.25Cr-1Mo plate used in power plant, refinery pipework and pressure vessels.

The chromium and molybdenum help the weld keep its strength at high service temperatures. It is not a general-purpose steel rod, so use it where the drawing, code or welding procedure calls for a matching 2.25Cr-1Mo filler.

Which base metals does it match, and what about dissimilar joints?icon-minus-redicon-plus-red

It is chosen to match 2.25Cr-1Mo steels, for example P22 pipe and the equivalent plate grades. Other creep-resistant steels have their own matching fillers, so do not assume one rod fits them all.

For dissimilar joints, the filler normally matches the less highly alloyed of the two steels, but the final choice should come from your qualified welding procedure and the applicable code. If you are unsure, check with your welding engineer before buying.

How does ER90S-B3 differ from ER80S-B2 and ER90S-B9?icon-minus-redicon-plus-red

The difference is mainly the chromium and molybdenum content, which sets the base metal each one matches. ER80S-B2 is a lower-alloy wire (about 1.25% chromium, 0.5% molybdenum) for steels such as P11. ER90S-B3 steps up to about 2.25% chromium and 1% molybdenum for P22. ER90S-B9 is in a different class altogether, with about 9% chromium, for P91-type steels.

They are not interchangeable. Using a lower-alloy filler on P22, or the reverse, is generally not accepted on code work without engineering approval.

Do I need to preheat before welding with it?icon-minus-redicon-plus-red

Yes. Chromium-molybdenum creep-resistant steels are prone to hydrogen cracking, so preheat is normally essential, and the interpass temperature is kept below a set maximum. The minimum preheat usually rises with thickness.

The correct figures for your job depend on thickness, joint and the code, so always follow your qualified welding procedure. Keep the joint at temperature between passes, and do not let it cool to room temperature part-way through unless the procedure allows it.

Does the weld need post-weld heat treatment?icon-minus-redicon-plus-red

Almost always. Post-weld heat treatment is mandatory in most application codes for creep-resistant steels. It softens the hard as-welded structure, improves toughness and sets up the carbide structure needed for long-term creep strength. The temperature and hold time come from the procedure and code, so do not take figures from a rod description.

Plan the heat treatment before you start welding, because it affects when the joint can be released and inspected.

Why do data sheets for this wire quote an X factor or low impurity levels?icon-minus-redicon-plus-red

In 2.25Cr-1Mo weld metal, trace impurities such as phosphorus, tin, antimony and arsenic can gather at grain boundaries during long periods in the 400 to 600 degrees C range. This is called temper embrittlement, and it makes the weld less tough. The X factor is a calculation from these impurities, and a lower figure means lower risk.

A low-impurity wire with a stated X factor limit is therefore chosen for pressure equipment that will run hot for years. If your specification sets a limit, check the wire's certificate to confirm it meets it.