Spot Welders FAQs
Straight answers to the questions people ask most when choosing and using a resistance spot welder.
What materials and thicknesses can a spot welder join?

Spot welding is mainly used on sheet metal, especially low-carbon steel, and also on stainless steel and coated steels. The thickness it can join depends on the machine, mainly its power rating, electrode force and arm size. Larger machines handle thicker sheet.
Aluminium and copper alloys conduct electricity and heat so well that they need much higher current and often a machine designed for them, so a general steel machine may not suit. Coated or galvanised steel usually needs more current or force, and more electrode care. The maker's data sheet states the thicknesses a machine can handle.
What types of spot welder are there?

Hand-held spot welding guns are portable and are used for repair and light work where you take the gun to the job. Station machines have fixed arms and the work is brought to them, which gives consistent results on repeat jobs. Larger industrial machines, often operated by foot pedal or by compressed air, handle thicker or higher-volume production work. Inverter (medium frequency) machines use electronic control to give precise, efficient control of the weld current and are used for demanding work.
Choose by the material, thickness, volume of work and whether it is easier to move the gun or the work.
What do the kVA rating, arm length and throat depth tell me?

The kVA rating shows the machine's power capacity and is a rough guide to the thickness it can weld: a higher rating suits thicker or tougher work. The arms carry the current to the electrodes. Their length sets the throat depth, which is how far in from the edge of a panel you can reach, and the gap between the arms sets the height of work you can fit.
Longer arms give more reach but may reduce the current that reaches the weld, so choose arms no longer than the job needs. The data plate and manual state the arm options and the thickness the machine can weld.
What settings control the quality of a spot weld?

Three things matter most: the welding current, the weld time and the electrode force. Too little current or time gives a weak weld or none, while too much causes burn-through, splashing of molten metal and marked surfaces. Too little force can cause spitting and a poor weld, and too much can squeeze the sheets and shorten electrode life.
Many machines also control a squeeze time before the current flows and a hold time afterwards, while the weld cools under pressure. Start from the maker's guidance for your material and thickness, make test welds on offcuts and adjust one setting at a time.