    UTP 83 FN Cast Iron Electrodes 3.2mm Diameter x 350mm Long. 1.4kg Pack (46 Rods). E NiFe-Cl
    52646

    £93.34  EX VAT
    SSP Suggested Selling Price = £106.15  YOU SAVE £12.81
     Buy in 3 easy interest free payments of £31.11† with

    UTP 83 FN is suitable for surfacing and joining all commercial cast iron grades, such as lamellar grey cast iron and nodular cast iron, malleable cast iron and for joining these materials to steel or cast steel. This stick electrode is particularly used where a high deposition rate is needed. UTP 83 FN has an excellent melting performance, and the easily controllable transfer provides a spatter-free deposit of perfect appearance. The weld deposit is easily machinable with cutting tools, tough and crack-resistant.

    Classifications
    EN ISO 1071: E C NiFe-11
    AWS A5.15: E NiFe-Cl

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Cast Iron Electrodes FAQs

    Straight answers to the questions buyers ask most when choosing and using electrodes for repairing and joining cast iron.

    How do I know what type of cast iron I am welding?icon-minus-redicon-plus-red

    The type matters because it decides how likely the casting is to crack. Grey iron is the most brittle, nodular (ductile) iron is more forgiving, and white iron is normally considered unweldable. Where possible, check the original drawing or specification.

    Simple workshop checks can give a hint but are not definitive: grey iron often leaves a dark graphite smudge when ground or scratched, tends to chip rather than curl under a sharp chisel, and does not ring when struck. These tests do not reliably tell ductile iron from steel, so if the casting is critical, have it identified properly.

    How should I prepare a casting before welding it?icon-minus-redicon-plus-red

    Remove all paint, grease and oil from the area, and grind off the hard outer skin of the casting down to clean metal. Oil soaked into the iron over years of service can be a problem, so heat the area gently before welding to drive out trapped oil and moisture, and clean it again.

    If the repair is a crack, find where it ends and make sure it is completely removed or stopped, because any crack left behind can grow back through the new weld. Follow the maker's instructions and your own welding procedure.

    Do I need to preheat cast iron, and how should it cool?icon-minus-redicon-plus-red

    Preheating slows the cooling rate and reduces the stresses that cause cracking. How much is needed depends on the type of iron, the thickness and complexity of the casting and the electrode used. Some nickel electrodes can be used with little or no preheat on small, thin repairs, while larger or more complex castings usually need more.

    Heat slowly and evenly, because uneven heating can itself crack a casting. After welding, let it cool slowly, for example by covering it with an insulating blanket or dry sand, rather than quenching it. Check the maker's data sheet for the recommended temperatures.

    Why are short weld runs and peening recommended?icon-minus-redicon-plus-red

    Short stringer beads at low heat input keep the heated zone small and limit the build-up of shrinkage stress. Weld a short length, let the area cool until you can comfortably touch it, then continue, often jumping to a different place along the repair.

    Peening means lightly hammering each bead while it is still hot to relieve the shrinkage stress. It is only suitable with the soft, ductile nickel or nickel-based deposits, not with hard weld metal. Use a rounded peening tool and light blows, and follow the maker's instructions for the electrode.