    UTP AF Robotic 601, 1.2mm Hardfacing MIG Wire, 16Kg Reel, EN 14700
    38748

    £395.20  EX VAT
     Buy in 3 easy interest free payments of £131.73† with

    UTP AF ROBOTIC 601 is a seamless chromium-niobium alloyed metal-cored wire for hardfacing using Ar-CO² shielding gas, without slag. The hardfacing deposit yields a high hardness as a result of special carbides but remains crack-free. A buffer of UTP A 63 is only recommended for critical materials or multilayer build-up. In these cases, only the last two beads should be welded with UTP AF ROBOTIC 601. Well suited for wear-resisting parts subject to heavy impact and shock, as well as abrasion. Weld metal is machinable only by grinding.  

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Hard Facing MIG Wire FAQs

    Straight answers to the questions buyers ask most when choosing and using hardfacing cored wire for wear-resistant overlays.

    How do I choose the right hardfacing wire for my wear problem?icon-minus-redicon-plus-red

    Start by working out how the part wears. Sliding of loose material under low pressure (low-stress abrasion) usually calls for a harder deposit with plenty of carbides. Crushing and grinding under high pressure needs a tougher deposit with well-spread carbides. Heavy pounding or gouging usually points to a work-hardening austenitic manganese type, and metal-to-metal wear or galling suits a tool-steel type of deposit.

    Most real parts suffer a mix of wear types, so aim for the best balance rather than the hardest deposit. Check the base metal too, because it affects preheat and whether a buffer layer is needed. Our team can help you match a wire to the job.

    What is the difference between chromium carbide, martensitic and manganese hardfacing wires?icon-minus-redicon-plus-red

    Chromium carbide deposits are the usual choice for abrasion with low to moderate impact. They are very hard but brittle, so they tend to show fine cracks and are usually limited in how many layers can be built up.

    Martensitic deposits are a compromise: good abrasion resistance with better toughness, so they suit mixed abrasion and impact, and they are often used as a build-up as well. Austenitic manganese deposits are tough and harden under hammering, so they suit heavy impact and rebuilding manganese steel parts, but they are not the best choice for pure sliding abrasion. Always check the maker's data sheet for the alloy you are considering.

    Do I need a buffer layer before hardfacing?icon-minus-redicon-plus-red

    Often, yes. A buffer or build-up layer gives the hard deposit a tough, crack-resistant base, and it is commonly used on steels that harden easily and when rebuilding worn parts. The buffer must be compatible with both the base metal and the final hardfacing alloy.

    On manganese steel, an austenitic buffer is normally used rather than a carbon steel build-up. Before welding, remove the old work-hardened surface from manganese steel, because leaving it in place can cause cracking under the weld. If a wire's data sheet specifies a buffer layer for your base metal, follow it.

    Is it normal for a hardfacing deposit to crack?icon-minus-redicon-plus-red

    With chromium carbide types, fine cracks running across the beads (check cracking) are usually normal. They form as the hard, brittle deposit cools and contracts, and they relieve stress. They are generally not harmful to wear performance unless the part sees a corrosive service.

    Cracks that run along the bead, or that go down into the base metal (underbead cracking), are a warning sign. They can lead to the deposit breaking away. Common causes are too little dilution with the base metal, no buffer layer, too little preheat or cooling too quickly. If your deposit shows irregular cracking, review the procedure and the data sheet.