WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE

TIG 312

Description:

312 deposits a 29% Cr / 9% Ni austenitic / ferritic stainless steel weld metal with a ferrite content of about FN 40.  The weld metal exhibits excellent tolerance to dilution from dissimilar and difficult-to-weld base materials without hot cracking, together with high strength and very good heat and oxidation resistance.

Applications:

  • Difficult-to-weld steel e.g. high carbon hardenable tool, die and spring steel, 13% Mn steel, free-cutting steel, high temperature steel.
  • Surfacing of metal-to-metal wear areas, hot working tools, furnace components.
  • Buffer layers prior to hard facing with high chromium carbide deposits.
  • Dissimilar joints between stainless and high carbon steel.


Welding current: DC-
Wire composition, wt.%

  C Si Mn P S Cr Ni Mo Cu
Min   0,30 1,0     28,0 8,0    
Typical 0,10 0,50 1,9 0,020 0,015 30,5 9,2 0,10 0,10
Max 0,15 0,65 2,5 0,030 0,020 32,0 12,0 0,30 0,30

Tig 312 FAQs

Straight answers to the questions people ask most when choosing and using 312 stainless TIG wire.

What is 312 TIG wire used for?icon-minus-redicon-plus-red

312 is a high-alloy stainless filler (the ER312 class, roughly 29% chromium and 9% nickel) used where an ordinary stainless filler would struggle. Its typical jobs are joining stainless to carbon or low-alloy steel, welding difficult or unknown steels, repairing tools, shafts and springs, and laying a tough buffer layer before hard surfacing.

It gives a weld metal that is strong and tolerant of dilution from the other metal in the joint. It is a specialist filler rather than a general-purpose one, so for ordinary stainless-to-stainless work a matching filler is normally the better choice.

Should I use 312 or 309L to join stainless steel to carbon steel?icon-minus-redicon-plus-red

Both are widely used for dissimilar joints. 309L is usually the first choice for stainless to carbon or low-alloy steel, because it is designed to cope with the carbon steel diluting the weld pool. 312 carries even more alloy and a higher ferrite content, so it is often chosen when dilution is heavy, when the carbon steel is hard to weld, or when a stronger weld metal is wanted.

Neither filler removes the narrow hard layer that can form next to the carbon steel, so keep dilution low and follow your welding procedure. If the joint has a specification, use the filler it names.

Why does 312 resist cracking on difficult steels?icon-minus-redicon-plus-red

312 weld metal solidifies with a high proportion of ferrite in an austenitic structure. Ferrite absorbs impurities such as sulphur and phosphorus more readily than austenite, which makes solidification cracking much less likely. That is why this type of filler is recommended when the base metal is high in carbon, sulphur or alloying elements, or when you are not sure of its composition.

The benefit has limits. Very high ferrite can reduce toughness and cause trouble at high temperatures, so 312 is not the answer to every cracking problem. Good fit-up, clean surfaces and sensible heat input still matter.

Can I weld tool steel or other hardenable steel with 312 and no preheat?icon-minus-redicon-plus-red

Not safely as a rule. Tool, die and spring steels have a high carbon content and crack easily, and the usual advice is to preheat, keep the interpass temperature under control and cool slowly, or heat treat straight after welding. An austenitic filler such as 312 gives a tough, ductile weld metal that reduces the cracking risk where full preheat is impractical, but the hard heat-affected zone in the parent steel is still at risk.

The weld metal will also not harden like the tool steel, so it suits repairs and build-up rather than parts needing full hardness. Follow the steel maker's guidance and your risk assessment.

Can 312 be used for high-temperature service?icon-minus-redicon-plus-red

Use caution. Ferrite-rich weld metal can become brittle if it is held for long periods at high temperature. At a few hundred degrees C it can suffer 475 degree embrittlement, and at higher temperatures brittle sigma phase can form, with more ferrite meaning more risk. Both effects reduce toughness.

So 312 is well suited to dissimilar joints and surfacing that run hot only occasionally, but it is not an automatic choice for long-term high-temperature duty. Check the maker's stated service limit for the wire and the requirements of your application before you choose it.

Can I use 312 on free-cutting steel?icon-minus-redicon-plus-red

Free-cutting and free-machining steels contain added sulphur, which forms low-melting films at the grain boundaries and makes them prone to cracking and porosity when welded. The usual advice is to avoid welding them where possible, ideally by choosing a different steel at the design stage.

If welding cannot be avoided, some welders try a high-ferrite stainless filler such as 312 with low heat input and light, clean passes, but this is not a guaranteed fix and cracking is still likely. Test on a sample first, follow the steel maker's advice and a qualified procedure, and do not use the joint on a safety-critical part unless it has been properly qualified.

Can I use 312 as a buffer layer before hard facing?icon-minus-redicon-plus-red

That is one of its common uses. A tough, work-hardening austenitic layer between a soft or crack-prone base metal and a very hard overlay helps stop cracks running into the parent steel. Makers of this type of wire list buffer layers under hard facing, and weld repairs on manganese steels, among its applications.

Other austenitic fillers such as 309L are also used for this job, so check what the hard-facing consumable's maker recommends. Keep heat input moderate, and on work-hardened parent metal remove the hardened surface layer before building up, as the data sheet for your hard-facing consumable will explain.