    ESAB OK Tigrod 316L Stainless Steel TIG Wire, 1000mm Cut Lengths - AWS A5.9 ER316L, 5Kg Pack
    1630XXR150

    Select Option 
    Prices From £68.50 ex VAT

    OK Tigrod 316L, a bare corrosion-resisting chromium-nickel-molybdenum welding rod, is a reliable choice for the welding of austenitic stainless alloys of 18% Cr - 8% Ni and 18% Cr - 10% Ni - 3% Mo types. It offers good general corrosion resistance, particularly against corrosion in acid and chlorinated environments. The low carbon content of the alloy reduces the risk of intergranular corrosion, further enhancing its reliability. This product is widely trusted in chemical and food processing, shipbuilding, and architectural structures.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig 316L / Lsi FAQs

    Straight answers to the questions people ask most when choosing and using 316L and 316LSi stainless steel TIG wire.

    What is the difference between 316L and 316LSi wire?icon-minus-redicon-plus-red

    316LSi has a higher silicon content than plain 316L. Filler makers say this improves wetting and gives a smoother bead. Otherwise both are low-carbon, molybdenum-bearing fillers for 316 and 316L base metals, and both are used with pure argon.

    On the pack, 316L is shown as ER316L in the American system or 19 12 3 L in the European system, and the Si type carries an Si suffix. Always check that the classification matches your specification or procedure.

    Why is the carbon content low in 316L?icon-minus-redicon-plus-red

    When stainless steel sits in a certain elevated temperature range, as the heat-affected zone of a weld does, chromium can be tied up with carbon at the grain boundaries. This is called sensitisation, and it can lower corrosion resistance. Low-carbon grades such as 316L are preferred for the best corrosion resistance, and the consumable should be low in carbon too.

    Low carbon reduces the risk rather than removing it, so control heat input and follow the specification for your application.

    Which polarity and shielding gas should I use?icon-minus-redicon-plus-red

    Stainless steel is TIG welded on DC with the electrode negative (DCEN), which is the usual polarity for stainless and other steels. This gives little cleaning of the surface, so the joint needs to be clean before you start.

    Filler makers specify pure argon as the shielding gas for 316L and 316LSi rod. Use a gas shield suited to the job, keep the flow steady and avoid draughts. Check your machine maker's guidance and your welding procedure for current, flow rate and any gas additions.

    Can I use 316L wire on 304 stainless?icon-minus-redicon-plus-red

    There is no 304 filler, so 304 is generally welded with a 308-type filler, and that is the usual match. 316L filler has a different composition, so do not assume it is a substitute. If your specification or a welding engineer calls for it, that is a different matter.

    Do not use it to join stainless to mild steel without advice. That type of joint generally needs an over-alloyed filler chosen for dissimilar metals, and your procedure should say which.