WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE

TIG 316L / LSI

Description:

316L is primarily intended for welding the low carbon, molybdenum alloyed, acid-resisting 316L austenitic stainless steels of similar composition.  Suitable also for welding 316 grades as well as Nb or Ti stabilised steels provided service temperatures for structural work are below 400°c.

Welding current: DC-
Wire composition, wt.%

  C Si Mn P S Cr Ni Mo Cu N
Min   0,30 1,0     18,0 11,0 2,5    
Typical 0,015 0,40 1,7 0,020 0,010 18,5 12,0 2,6 0,10 0,06
Max 0,030 0,65 2,5 0,030 0,020 20,0 14,0 3,0 0,30  

 

Tig 316L / Lsi FAQs

Straight answers to the questions people ask most when choosing and using 316L and 316LSi stainless steel TIG wire.

What is 316L TIG wire used for?icon-minus-redicon-plus-red

316L is a low-carbon stainless filler containing molybdenum. It is used to weld 316 and 316L stainless steels, which are chosen where good resistance to corrosion in acid and chlorinated environments is needed. Filler makers list chemical and food processing plant and shipbuilding among the typical uses.

Use it when the base metal is 316 or 316L and the weld needs to match the parent metal's performance. For ordinary 304 stainless, a 308-type filler is the usual match.

What is the difference between 316L and 316LSi wire?icon-minus-redicon-plus-red

316LSi has a higher silicon content than plain 316L. Filler makers say this improves wetting and gives a smoother bead. Otherwise both are low-carbon, molybdenum-bearing fillers for 316 and 316L base metals, and both are used with pure argon.

On the pack, 316L is shown as ER316L in the American system or 19 12 3 L in the European system, and the Si type carries an Si suffix. Always check that the classification matches your specification or procedure.

Why is the carbon content low in 316L?icon-minus-redicon-plus-red

When stainless steel sits in a certain elevated temperature range, as the heat-affected zone of a weld does, chromium can be tied up with carbon at the grain boundaries. This is called sensitisation, and it can lower corrosion resistance. Low-carbon grades such as 316L are preferred for the best corrosion resistance, and the consumable should be low in carbon too.

Low carbon reduces the risk rather than removing it, so control heat input and follow the specification for your application.

Which polarity and shielding gas should I use?icon-minus-redicon-plus-red

Stainless steel is TIG welded on DC with the electrode negative (DCEN), which is the usual polarity for stainless and other steels. This gives little cleaning of the surface, so the joint needs to be clean before you start.

Filler makers specify pure argon as the shielding gas for 316L and 316LSi rod. Use a gas shield suited to the job, keep the flow steady and avoid draughts. Check your machine maker's guidance and your welding procedure for current, flow rate and any gas additions.

Do I need to back-purge stainless steel welds?icon-minus-redicon-plus-red

Where the inside of a full-penetration weld will be exposed to heat, such as on tube, the root side oxidises unless you shield it. The resulting heat-tint is a chromium-rich scale that gives little protection and leaves the surface short of chromium, which can reduce corrosion resistance. Pure argon is the recommended backing gas.

Keep the purge on until the root and hot pass are complete, and sometimes the first few fill passes. Argon is heavier than air and can build up in enclosed spaces, so follow HSE guidance on asphyxiation hazards and avoid entering confined spaces.

Can I use 316L wire on 304 stainless?icon-minus-redicon-plus-red

There is no 304 filler, so 304 is generally welded with a 308-type filler, and that is the usual match. 316L filler has a different composition, so do not assume it is a substitute. If your specification or a welding engineer calls for it, that is a different matter.

Do not use it to join stainless to mild steel without advice. That type of joint generally needs an over-alloyed filler chosen for dissimilar metals, and your procedure should say which.