WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : 2594  

    IABCO High Nickel Tig Wire, 1000mm Cut Lengths - AWS A5.9 ER2594. 5Kg Pack
    2594

    Select Option 
    Prices From £241.38 ex VAT

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    High Nickel TIG Wire FAQs

    Straight answers to the questions people ask most when choosing and using nickel alloy TIG filler wire.

    Why does cleanliness matter so much with nickel alloys?icon-minus-redicon-plus-red

    Nickel alloys are easily embrittled at high temperature by sulphur, lead, phosphorus, boron and bismuth. These can come from oils, grease, cutting fluids, paints, marker pens and temperature-indicating crayons. Contamination of this kind can cause cracking in the weld or heat-affected zone.

    Keep the joint, the filler wire and your tools free of these materials, and use brushes and tools kept only for nickel alloys. Avoid marking with ordinary markers or crayons near the weld.

    How should I prepare nickel alloy before welding?icon-minus-redicon-plus-red

    Degrease the joint area first, remove the surface oxide by machining, grinding or a similar method, and then degrease again to remove anything introduced during cleaning. Wire brushing alone is usually not enough, because it tends to polish the oxide rather than remove it.

    Between passes, remove oxide as well, as it can cause inclusions and lack of fusion. Weld soon after cleaning, and keep the cleaning tools dedicated to nickel alloys.

    Which shielding gas should I use for TIG welding nickel alloys?icon-minus-redicon-plus-red

    Pure argon is the usual choice, and argon with helium or with a small addition of hydrogen is also used for some alloys. A hydrogen addition can improve the fluidity of the weld pool and give cleaner welds, but it is not suitable for every alloy, so check the filler maker's recommendation.

    Good gas coverage matters, because oxygen and nitrogen from the air cause porosity. Keep gas hoses in good condition, avoid draughts, and use a back purge where the root side of the joint needs protecting.

    Why does a nickel filler get used to join stainless steel to carbon steel?icon-minus-redicon-plus-red

    Nickel alloy fillers generally perform well in dissimilar joints between ferritic and austenitic steels. The thermal expansion of nickel alloys sits between that of ferritic steel and austenitic stainless steel, so the joint suffers less thermal fatigue when it heats and cools repeatedly.

    The right nickel filler for a dissimilar joint depends on the metals and the service conditions, such as temperature and corrosion. Check the filler maker's data sheet and, for critical work, the specification you are working to.