WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : 60024  

    Lincoln LNT 20 Steel TIG Wire, 1000mm Cut Lengths, 5Kg Pack, AWS A5.28 ER90S-B3
    60024

    Select Option 
    Prices From £71.48 ex VAT

    Solid rod for welding creep and hydrogen resistant Cr-Mo steels (2,25Cr - 1Mo).  Service temperature up to 600°c.

    Classification
    AWS A5.28 - ER90S-B3 Nearest classification
    ISO 21952-A - W CrMo2Si

    Shielding Gas
    l1 Inert gas AR (100%)

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig Er90S-B3 FAQs

    Straight answers to the questions people ask most when choosing and using 2.25Cr-1Mo chromium-molybdenum TIG filler wire.

    What is ER90S-B3 TIG wire used for?icon-minus-redicon-plus-red

    ER90S-B3 is a low-alloy chromium-molybdenum solid rod, classed under the American standard for low-alloy steel filler rods. It contains roughly 2.25% chromium and 1% molybdenum, and it is used to weld creep-resistant steels of the same type, such as P22 pipe and 2.25Cr-1Mo plate used in power plant, refinery pipework and pressure vessels.

    The chromium and molybdenum help the weld keep its strength at high service temperatures. It is not a general-purpose steel rod, so use it where the drawing, code or welding procedure calls for a matching 2.25Cr-1Mo filler.

    How does ER90S-B3 differ from ER80S-B2 and ER90S-B9?icon-minus-redicon-plus-red

    The difference is mainly the chromium and molybdenum content, which sets the base metal each one matches. ER80S-B2 is a lower-alloy wire (about 1.25% chromium, 0.5% molybdenum) for steels such as P11. ER90S-B3 steps up to about 2.25% chromium and 1% molybdenum for P22. ER90S-B9 is in a different class altogether, with about 9% chromium, for P91-type steels.

    They are not interchangeable. Using a lower-alloy filler on P22, or the reverse, is generally not accepted on code work without engineering approval.

    Does the weld need post-weld heat treatment?icon-minus-redicon-plus-red

    Almost always. Post-weld heat treatment is mandatory in most application codes for creep-resistant steels. It softens the hard as-welded structure, improves toughness and sets up the carbide structure needed for long-term creep strength. The temperature and hold time come from the procedure and code, so do not take figures from a rod description.

    Plan the heat treatment before you start welding, because it affects when the joint can be released and inspected.

    Why do data sheets for this wire quote an X factor or low impurity levels?icon-minus-redicon-plus-red

    In 2.25Cr-1Mo weld metal, trace impurities such as phosphorus, tin, antimony and arsenic can gather at grain boundaries during long periods in the 400 to 600 degrees C range. This is called temper embrittlement, and it makes the weld less tough. The X factor is a calculation from these impurities, and a lower figure means lower risk.

    A low-impurity wire with a stated X factor limit is therefore chosen for pressure equipment that will run hot for years. If your specification sets a limit, check the wire's certificate to confirm it meets it.