    Nickel Alloy 59 TIG Wire, 1000mm Cut Lengths - AWS A5.14 ER NiCrMo-13, 5Kg Pack
    601110060

    Select Option 
    Prices From £542.50 ex VAT

    • Alloy 59 is a nickel-chromium-molybdenum alloy with an extra low carbon and silicon content.
    • Versatile alloy with excellent wet corrosion resistance for the most demanding applications.
    • The high level of Mo is similar to alloy C276 but performs better in a wider range of oxidising media’s.
    • Typically used in the welding of aggressively corrosive media’s, including scrubbers for flue gas desulphurisation, digesters and papermaking equipment, chemical process plants, corrosion resistant overlays and in severe offshore and petrochemical industries etc.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    High Nickel TIG Wire FAQs

    Straight answers to the questions people ask most when choosing and using nickel alloy TIG filler wire.

    How do I choose the right nickel alloy TIG filler?icon-minus-redicon-plus-red

    Start from the base metal. For most nickel alloys the filler is chosen to match the parent metal, for example a pure nickel rod for commercial purity nickel and a nickel-chromium-molybdenum rod for the matching alloy 625 type. Many fillers contain small additions such as titanium, aluminium or niobium to reduce porosity and cracking.

    The filler is named by its class, such as the American ERNi- or ERNiCr- designations, so check that class against the maker's data sheet and the specification or procedure for your job. If you are joining two different metals, the filler needs to suit both.

    Why does cleanliness matter so much with nickel alloys?icon-minus-redicon-plus-red

    Nickel alloys are easily embrittled at high temperature by sulphur, lead, phosphorus, boron and bismuth. These can come from oils, grease, cutting fluids, paints, marker pens and temperature-indicating crayons. Contamination of this kind can cause cracking in the weld or heat-affected zone.

    Keep the joint, the filler wire and your tools free of these materials, and use brushes and tools kept only for nickel alloys. Avoid marking with ordinary markers or crayons near the weld.

    Which shielding gas should I use for TIG welding nickel alloys?icon-minus-redicon-plus-red

    Pure argon is the usual choice, and argon with helium or with a small addition of hydrogen is also used for some alloys. A hydrogen addition can improve the fluidity of the weld pool and give cleaner welds, but it is not suitable for every alloy, so check the filler maker's recommendation.

    Good gas coverage matters, because oxygen and nitrogen from the air cause porosity. Keep gas hoses in good condition, avoid draughts, and use a back purge where the root side of the joint needs protecting.

    Why does a nickel filler get used to join stainless steel to carbon steel?icon-minus-redicon-plus-red

    Nickel alloy fillers generally perform well in dissimilar joints between ferritic and austenitic steels. The thermal expansion of nickel alloys sits between that of ferritic steel and austenitic stainless steel, so the joint suffers less thermal fatigue when it heats and cools repeatedly.

    The right nickel filler for a dissimilar joint depends on the metals and the service conditions, such as temperature and corrosion. Check the filler maker's data sheet and, for critical work, the specification you are working to.