WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : 68442  

    Bohler Fox DCMS Kb Electrodes 3.2mm, 4.1kg E8018-B2
    68442

    £77.15  EX VAT
    SSP Suggested Selling Price = £97.17  YOU SAVE £20.02
     Buy in 3 easy interest free payments of £25.72† with

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Bohler Low Hydrogen FAQs

    Straight answers to the questions people ask most when choosing and using low hydrogen stick electrodes for mild, higher strength and chrome-moly steels.

    How low does the hydrogen level need to be for thick or high strength steel?icon-minus-redicon-plus-red

    The lower the diffusible hydrogen, the lower the cracking risk, and the requirement gets tighter as the steel gets stronger, thicker or more restrained. For many ordinary jobs a low hydrogen basic electrode is enough, but for high restraint, heavy sections or alloyed weld metal, stricter hydrogen limits and preheat may be required.

    Hydrogen levels are graded in standard scales running from high to ultra-low, and a lower marking such as H4 means a tighter limit than H8. Your procedure should say what grade is needed; choose an electrode marked to meet it.

    When must I bake low hydrogen electrodes, and can I over-bake them?icon-minus-redicon-plus-red

    Basic electrodes should be baked according to the manufacturer's instructions unless they come in sealed packaging that is opened just before use. After baking, keep them warm in a holding oven or limit the time they sit in the open to the maker's stated time.

    Baking is not unlimited. Repeated or excessive drying can damage the coating, making it crumble or come away, and many makers limit the number of re-bakes. Follow the temperature, time and number of cycles on the pack or data sheet rather than a figure from another electrode.

    What is an E8018-B2 type electrode used for?icon-minus-redicon-plus-red

    This type is a low hydrogen electrode with chromium and molybdenum in the deposit, designed to match 1.25Cr-0.5Mo creep-resistant steels such as those used in pipework and pressure parts running at raised temperatures. The alloy gives the weld strength and resistance to creep and oxidation at heat.

    Because the weld metal is alloyed, it is more sensitive to hydrogen cracking than plain mild steel, so careful storage, preheat and usually post-weld heat treatment apply. Always use the electrode named in the welding procedure, and check the maker's data sheet for the exact temperatures and conditions.

    What is the difference between vacuum-packed, tin and sealed low hydrogen electrodes?icon-minus-redicon-plus-red

    All of them are ways of keeping basic coatings dry until you open them. Vacuum packs and sealed tins protect the electrodes from moisture in the air, so they can often be used straight from the pack without baking if the package is intact and they are used within the exposure time the maker gives.

    Once a pack is opened, the clock starts. Check that the pack is undamaged before use, as a torn or punctured pack should be treated as open. Electrodes left out beyond the maker's time need re-drying as instructed. The packaging type and exposure time vary, so read the label.