    UTP 8 Cast Iron Electrodes 3.2mm Diameter x 350mm Long. 2.1kg Pack. E Ni-Cl
    89434

    £103.76  EX VAT
    SSP Suggested Selling Price = £166.65  YOU SAVE £62.89
     Buy in 3 easy interest free payments of £34.59† with
    UTP 8 is for cold welding of grey and malleable cast iron and cast steel and for joining these base metals to steel, copper and copper alloys, especially for repair and maintenance. UTP 8 has excellent welding properties. The easily controllable flow permits spatter-free welding in all positions and with minimal amperage. The weld deposit and the transition zones are fillable. No undercutting. Ideally suited for the combined welding with the ferro-nickel type UTP 86 FN (buttering with UTP 8 and filling with UTP 86 FN).

    Classifications
    EN ISO 1071: E C Ni-Cl 1
    AWS A5.15: E Ni-Cl

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Cast Iron Electrodes FAQs

    Straight answers to the questions buyers ask most when choosing and using electrodes for repairing and joining cast iron.

    What are cast iron electrodes used for?icon-minus-redicon-plus-red

    They are coated electrodes for the manual metal arc process, used to repair cracked or broken castings and to join cast iron to itself or to other metals. Most are nickel-based, because a nickel deposit stays relatively soft and ductile even when it picks up carbon from the casting.

    Cast iron is difficult to weld because its high carbon content can make the weld and the zone beside it hard and brittle, which leads to cracking as it cools. Treat every cast iron repair as a job that needs care and a plan, not a quick tack.

    Should I choose a pure nickel or a nickel-iron electrode?icon-minus-redicon-plus-red

    Pure nickel types (often classed as ENi-CI) generally give the softest, most machinable deposit and suit repairs where you need to drill, tap or file the weld afterwards. Nickel-iron types (often classed as ENiFe-CI) are generally stronger and tolerate dilution from the casting better, so they suit thicker sections, higher-strength irons and joining cast iron to steel.

    If the grade of iron is unknown, a nickel-copper type is sometimes used instead. Check the maker's data sheet for the electrode's intended use, and our team can help you choose.

    How should I prepare a casting before welding it?icon-minus-redicon-plus-red

    Remove all paint, grease and oil from the area, and grind off the hard outer skin of the casting down to clean metal. Oil soaked into the iron over years of service can be a problem, so heat the area gently before welding to drive out trapped oil and moisture, and clean it again.

    If the repair is a crack, find where it ends and make sure it is completely removed or stopped, because any crack left behind can grow back through the new weld. Follow the maker's instructions and your own welding procedure.

    Do I need to preheat cast iron, and how should it cool?icon-minus-redicon-plus-red

    Preheating slows the cooling rate and reduces the stresses that cause cracking. How much is needed depends on the type of iron, the thickness and complexity of the casting and the electrode used. Some nickel electrodes can be used with little or no preheat on small, thin repairs, while larger or more complex castings usually need more.

    Heat slowly and evenly, because uneven heating can itself crack a casting. After welding, let it cool slowly, for example by covering it with an insulating blanket or dry sand, rather than quenching it. Check the maker's data sheet for the recommended temperatures.