    SIFSteel 312 Stainless Steel TIG Wire, 1000mm Cut Lengths - AWS A5.9 ER312. 1Kg Pack
    SIF-T312

    Select Option 
    Prices From £26.88 ex VAT

    This is a 29.9 stainless TIG filler rod, suitable for difficult-to-weld steels (Mn steels, tool and spring steels), also dissimilar materials. High resistance to weld metal cracking.

    Typical applications for this weld-all rod include joining hard manganese steels, tool steels, spring steels, buffering as well as joining dissimilar steel grades. It deposits a crack-resistant weld metal with an increased ferrite content.  Base materials to be welded: Armour plate, hardenable steels including DFTW-steels, tool, die and spring steels, austenitic manganese steels, hardfacing clutches, gear wheels, shafts, buffer layers prior to hardfacing, dissimilar joining.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig 312 FAQs

    Straight answers to the questions people ask most when choosing and using 312 stainless TIG wire.

    Should I use 312 or 309L to join stainless steel to carbon steel?icon-minus-redicon-plus-red

    Both are widely used for dissimilar joints. 309L is usually the first choice for stainless to carbon or low-alloy steel, because it is designed to cope with the carbon steel diluting the weld pool. 312 carries even more alloy and a higher ferrite content, so it is often chosen when dilution is heavy, when the carbon steel is hard to weld, or when a stronger weld metal is wanted.

    Neither filler removes the narrow hard layer that can form next to the carbon steel, so keep dilution low and follow your welding procedure. If the joint has a specification, use the filler it names.

    Can I weld tool steel or other hardenable steel with 312 and no preheat?icon-minus-redicon-plus-red

    Not safely as a rule. Tool, die and spring steels have a high carbon content and crack easily, and the usual advice is to preheat, keep the interpass temperature under control and cool slowly, or heat treat straight after welding. An austenitic filler such as 312 gives a tough, ductile weld metal that reduces the cracking risk where full preheat is impractical, but the hard heat-affected zone in the parent steel is still at risk.

    The weld metal will also not harden like the tool steel, so it suits repairs and build-up rather than parts needing full hardness. Follow the steel maker's guidance and your risk assessment.

    Can I use 312 on free-cutting steel?icon-minus-redicon-plus-red

    Free-cutting and free-machining steels contain added sulphur, which forms low-melting films at the grain boundaries and makes them prone to cracking and porosity when welded. The usual advice is to avoid welding them where possible, ideally by choosing a different steel at the design stage.

    If welding cannot be avoided, some welders try a high-ferrite stainless filler such as 312 with low heat input and light, clean passes, but this is not a guaranteed fix and cracking is still likely. Test on a sample first, follow the steel maker's advice and a qualified procedure, and do not use the joint on a safety-critical part unless it has been properly qualified.

    Can I use 312 as a buffer layer before hard facing?icon-minus-redicon-plus-red

    That is one of its common uses. A tough, work-hardening austenitic layer between a soft or crack-prone base metal and a very hard overlay helps stop cracks running into the parent steel. Makers of this type of wire list buffer layers under hard facing, and weld repairs on manganese steels, among its applications.

    Other austenitic fillers such as 309L are also used for this job, so check what the hard-facing consumable's maker recommends. Keep heat input moderate, and on work-hardened parent metal remove the hardened surface layer before building up, as the data sheet for your hard-facing consumable will explain.