    Bohler Thermanit GE-316L Stainless Steel TIG Wire, 1000mm Cut Lengths - AWS A5.9 ER316L, 5Kg Pack
    THERMANIT-GE316LTIG

    Select Option 
    Prices From £80.16 ex VAT

    Stainless; resistant to intercrystallite corrosion and wet corrosion up to 400°C (752°F). Corrosion resistance like matching low-carbon and stabilised austenitic 18/8 CrNiMo steels / cast steel grades. For joining and surfacing application with matching and similar – non-stabilised and stabilised – austenitic CrNi(N) and CrNiMo(N) steels and cast steel grades.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig 316L / Lsi FAQs

    Straight answers to the questions people ask most when choosing and using 316L and 316LSi stainless steel TIG wire.

    Why is the carbon content low in 316L?icon-minus-redicon-plus-red

    When stainless steel sits in a certain elevated temperature range, as the heat-affected zone of a weld does, chromium can be tied up with carbon at the grain boundaries. This is called sensitisation, and it can lower corrosion resistance. Low-carbon grades such as 316L are preferred for the best corrosion resistance, and the consumable should be low in carbon too.

    Low carbon reduces the risk rather than removing it, so control heat input and follow the specification for your application.

    Which polarity and shielding gas should I use?icon-minus-redicon-plus-red

    Stainless steel is TIG welded on DC with the electrode negative (DCEN), which is the usual polarity for stainless and other steels. This gives little cleaning of the surface, so the joint needs to be clean before you start.

    Filler makers specify pure argon as the shielding gas for 316L and 316LSi rod. Use a gas shield suited to the job, keep the flow steady and avoid draughts. Check your machine maker's guidance and your welding procedure for current, flow rate and any gas additions.

    Do I need to back-purge stainless steel welds?icon-minus-redicon-plus-red

    Where the inside of a full-penetration weld will be exposed to heat, such as on tube, the root side oxidises unless you shield it. The resulting heat-tint is a chromium-rich scale that gives little protection and leaves the surface short of chromium, which can reduce corrosion resistance. Pure argon is the recommended backing gas.

    Keep the purge on until the root and hot pass are complete, and sometimes the first few fill passes. Argon is heavier than air and can build up in enclosed spaces, so follow HSE guidance on asphyxiation hazards and avoid entering confined spaces.

    Can I use 316L wire on 304 stainless?icon-minus-redicon-plus-red

    There is no 304 filler, so 304 is generally welded with a 308-type filler, and that is the usual match. 316L filler has a different composition, so do not assume it is a substitute. If your specification or a welding engineer calls for it, that is a different matter.

    Do not use it to join stainless to mild steel without advice. That type of joint generally needs an over-alloyed filler chosen for dissimilar metals, and your procedure should say which.