WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : CK-2A4L  Mfr Ref : 2A4L

    CK Long Alumina Nozzle 6mm Bore A796F71
    2A4L CK-2A4L

    £12.95  EX VAT
    SSP Suggested Selling Price = £25.89  YOU SAVE £12.95

    Cup Alumina (1/4" X 1-7/8").

    Related Items

    • CK-2C4L Cup Ceramic 6.4mm

      Cup Ceramic 6.4mm

      Rapid ref : CK-2C4L
      Mfr Ref : 796F71
       


      £ 18.10 EX VAT
      YOU SAVE £ 18.09

    CK 2 Series Standard Parts FAQs

    Answers on choosing, fitting and looking after the standard collets, collet bodies, back caps and ceramic cups for a small TIG torch.

    In what order do I fit the parts, and how tight should the back cap be?icon-minus-redicon-plus-red

    The usual sequence is to screw the collet body (or gas lens) into the torch head, slide in the collet, fit the cup, then put the tungsten and back cap in from the rear. Do the final tightening of the back cap once the tungsten is in place.

    A welding-equipment maker's manual says to tighten the cap only until the tungsten can no longer be moved by hand, and to tighten the collet body or gas lens only lightly. It also warns that loose parts can cause poor arc starting. Always switch off and isolate the equipment before working on the torch, and follow the manual for your torch.

    Is grinding thoriated tungsten a health concern?icon-minus-redicon-plus-red

    Yes, grinding is the main hazard with thoriated electrodes because it creates fine, slightly radioactive dust that can be inhaled. Typical controls are a dedicated grinding wheel with local dust extraction, sealed bags for the dust and washing facilities nearby.

    Ceriated and lanthanated electrodes are common alternatives, especially for DC work, and zirconiated types are often used for AC. Your employer's risk assessment and the maker's instructions decide what is right for your work.

    Why is my tungsten loose or my arc wandering?icon-minus-redicon-plus-red

    Check the hardware first. A worn or wrong-size collet, a collet body that is not snug in the torch head or a loose back cap can all let the tungsten move. Replace worn or discoloured parts rather than over-tightening them.

    Then look at the electrode. A welding-equipment maker's data sheet advises grinding lengthways so that ridges do not cause arc wander, and its troubleshooting guide lists a contaminated electrode, too long an arc and too little current for the electrode size as causes of an erratic arc. Cut off and re-prepare a contaminated tip.

    When is it worth moving from a standard collet body to a gas lens?icon-minus-redicon-plus-red

    A standard collet body sends gas out through side holes, which can make the flow turbulent. A gas lens uses fine mesh screens to smooth it. A welding-equipment maker's troubleshooting guide suggests changing to gas lens or gas saver parts when poor shielding comes from turbulence or drafts.

    It usually helps most when you need a longer tungsten extension or better cover on stainless steel; with a very short extension you may see little difference. A gas lens needs its own compatible parts and cups, so it is not a simple swap. Check what your torch family accepts.

    Shop Similar Categories