WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : 1251086700  

    ESAB OK Autrod 12.51 0.8mm MIG Wire, 15Kg Reel, ER70S-6
    1251086700

    £99.65  EX VAT
    SSP Suggested Selling Price = £124.06  YOU SAVE £24.41
     Buy in 3 easy interest free payments of £33.22† with

    OK Autrod 12.51 is a copper-coated solid wire with higher levels of deoxidisers (manganese and silicon). The high content of deoxidisers allows welding over heavier amounts of dirt, rust, and mill scale while providing a more fluid puddle and smoother bead profile.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    ESAB Consumables FAQs

    Practical answers on choosing, storing and using welding wire and stick electrodes.

    How do I read the classification code on a stick electrode?icon-minus-redicon-plus-red

    Most stick electrodes carry a classification code on the pack, for example a letter E followed by digits. Taking a common low hydrogen code as an example: E means a stick electrode, the first two digits give the minimum tensile strength of the weld metal, the next digit shows the positions it can be used in, and the last digit tells you about the coating type and the current it needs. Extra suffixes can show a hydrogen limit or better impact toughness.

    Wire and rod codes follow their own patterns, so read the maker's data sheet or the standard named on the pack. Always match the code to the strength and type of the steel you are welding.

    How do I match a TIG filler rod to the metal I am welding?icon-minus-redicon-plus-red

    The weld pool is a mixture of the parent metal and the filler, so the rod is normally chosen to suit the parent metal. Carbon steel, low alloy steel and stainless each have their own rods, and low alloy heat-resistant steels need a rod made for that alloy. Using a general-purpose rod on everything is a common mistake.

    In TIG the filler is added to the weld pool by hand, separately from the arc, and argon is the usual gas for steels and stainless. Check the rod's data sheet or the standard named on its pack, and follow your welding procedure if the job is specified.

    Why are low hydrogen electrodes supplied in sealed packs?icon-minus-redicon-plus-red

    Low hydrogen electrodes are used where hydrogen cracking in the weld or heat affected zone must be avoided, such as on critical or more hardenable steels. Their coating picks up moisture from the air, which adds hydrogen to the weld. Sealed packs let you use them straight from the pack, with no baking needed beforehand.

    If a pack has been opened or damaged, the electrodes should be re-dried as the maker instructs and then kept warm or limited in their exposure time. Exact temperatures and times differ between makers, so follow the instructions on the pack and your job specification.

    Can I re-dry rutile or cellulosic electrodes if they get damp?icon-minus-redicon-plus-red

    These types are treated differently from low hydrogen ones. Rutile and cellulosic electrodes need some moisture in the coating to run properly, so they should not be baked. If rutile electrodes have become damp, gentle re-drying at the low temperature the maker states is generally enough. Some makers say cellulosic electrodes should not be re-dried at all, and electrodes that have been soaked are best thrown away.

    As the correct treatment depends on the electrode type and maker, check the pack or data sheet before using any heat on a damp electrode.

    Shop Similar Categories