    Rapid Ref : WER2493  

    ER80S-Ni1 Mig Wire 1.0mm Diameter x 15LKg Reel.
    WER2493

    £208.95  EX VAT
     Buy in 3 easy interest free payments of £69.65† with

    MIG ER80S-Ni FAQs

    Straight answers to the questions people ask most when choosing and using nickel-alloyed ER80S-Ni MIG wire.

    What is the difference between ER80S-Ni1 and ER80S-Ni2?icon-minus-redicon-plus-red

    The main difference is the nickel content. The classification for Ni1 calls for roughly 0.8 to 1.1% nickel, while Ni2 calls for roughly 2 to 2.75%. Higher nickel generally gives better toughness at very low temperatures, so Ni2 is aimed at colder service, while Ni1 suits moderately low temperatures.

    Both are in the same 80 ksi strength class. Note that the Ni1 range runs slightly above 1%, so if your specification sets a 1% nickel limit, such as for sour service, check the nickel figure on the batch certificate rather than relying on the class alone. Which wire you need depends on the lowest service temperature, the parent steel and the weld procedure.

    What does ER80S-Ni mean?icon-minus-redicon-plus-red

    It is a classification under the American standard for solid low-alloy steel wire used with gas shielding. The R shows it can be used as a rod or an electrode, the 80 means weld metal of about 80 ksi (550 MPa) minimum tensile strength, and the S means a solid wire. Ni shows that nickel is added deliberately.

    The number after Ni, such as Ni1 or Ni2, shows the nickel level band. The wire is made for good toughness at low temperature, so it is used on offshore, pipework and similar demanding jobs. Always check the wire's certificate for the exact class it meets.

    Do I need to preheat when using ER80S-Ni wire?icon-minus-redicon-plus-red

    It depends on the parent steel, thickness, restraint and the hydrogen level of the process. Preheat slows cooling, lets hydrogen escape and reduces hardness, which lowers the risk of hydrogen cracking.

    For low carbon-equivalent steels preheat is generally not needed if a low hydrogen process is used, but thick or highly restrained joints may need it, and higher carbon-equivalent steels need it more often. The joint must also be clean and dry. Follow the welding procedure for preheat and interpass temperatures rather than guessing from the wire alone.

    Which shielding gas should I use with ER80S-Ni wire?icon-minus-redicon-plus-red

    Use the gas listed on the wire's data sheet and in your welding procedure, usually an argon-rich mixture. Gas choice affects arc, spatter, penetration and toughness.

    Gas suppliers explain that adding oxygen or carbon dioxide raises the oxidation potential of the gas. For a given wire, the higher that is, the lower the strength and toughness of the weld, because oxide inclusions increase and manganese and silicon are lost. Where impact toughness matters, do not change the gas or flow rate from the approved procedure without checking with the welding engineer.

    Shop Similar Categories