    A5.28: ER 80S-Ni2ISO 14341: G 46 6 M G2Ni2. Solid wire for welding fine-grained and low-alloyed nickel steels.  High impact value at low temperature (-60°c as welded and -90°c after stress relieving 15h / 580°c).  Typical offshore applications.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    MIG ER80S-Ni FAQs

    Straight answers to the questions people ask most when choosing and using nickel-alloyed ER80S-Ni MIG wire.

    What is the difference between ER80S-Ni1 and ER80S-Ni2?icon-minus-redicon-plus-red

    The main difference is the nickel content. The classification for Ni1 calls for roughly 0.8 to 1.1% nickel, while Ni2 calls for roughly 2 to 2.75%. Higher nickel generally gives better toughness at very low temperatures, so Ni2 is aimed at colder service, while Ni1 suits moderately low temperatures.

    Both are in the same 80 ksi strength class. Note that the Ni1 range runs slightly above 1%, so if your specification sets a 1% nickel limit, such as for sour service, check the nickel figure on the batch certificate rather than relying on the class alone. Which wire you need depends on the lowest service temperature, the parent steel and the weld procedure.

    Why is the nickel limit of 1% so important for oil and gas work?icon-minus-redicon-plus-red

    For sour service, where hydrogen sulphide is present, the sour service standard requires sulphide stress cracking testing for carbon-manganese steel welds with more than 1% nickel in the deposit. Nickel is therefore generally kept to 1% maximum on such work, which is why a wire with a controlled nickel level is chosen.

    Some specifications allow a higher figure when it has been specially tested. Whether it applies to your job depends on the project specification and the current edition of the standard, so check those and the wire's certificate rather than assuming.

    When do I need a nickel wire instead of a standard steel wire?icon-minus-redicon-plus-red

    A standard mild steel wire is fine for general work, but plain carbon-manganese gas-shielded wires may not give adequate weld metal toughness at low temperatures such as -50 degrees C. Nickel is then usually needed to provide the required as-welded toughness.

    Nickel wires are therefore chosen when the specification calls for low-temperature impact toughness, such as offshore structures, pipework and cold-climate equipment. Makers also list them for sour-service work and some weathering steels. If your drawing or welding procedure names the filler, use that. If not, ask the designer or welding engineer.

    Which shielding gas should I use with ER80S-Ni wire?icon-minus-redicon-plus-red

    Use the gas listed on the wire's data sheet and in your welding procedure, usually an argon-rich mixture. Gas choice affects arc, spatter, penetration and toughness.

    Gas suppliers explain that adding oxygen or carbon dioxide raises the oxidation potential of the gas. For a given wire, the higher that is, the lower the strength and toughness of the weld, because oxide inclusions increase and manganese and silicon are lost. Where impact toughness matters, do not change the gas or flow rate from the approved procedure without checking with the welding engineer.