    • Alloy 617 is a high temperature wire used for welding of nickel chromium-cobalt-molybdenum alloys.
    • Ideal for overlay cladding where similar alloy is required, such as gas turbines and ethylene equipment.
    • Suitable for joining dissimilar alloys where high temperature strength and oxidation resistance are required up to about 1150°C.
    • Typically used in the aerospace and power generation industries, including petrochemical plants for applications such as nitric acid catalyst grids etc.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    High Nickel TIG Wire FAQs

    Straight answers to the questions people ask most when choosing and using nickel alloy TIG filler wire.

    How do I choose the right nickel alloy TIG filler?icon-minus-redicon-plus-red

    Start from the base metal. For most nickel alloys the filler is chosen to match the parent metal, for example a pure nickel rod for commercial purity nickel and a nickel-chromium-molybdenum rod for the matching alloy 625 type. Many fillers contain small additions such as titanium, aluminium or niobium to reduce porosity and cracking.

    The filler is named by its class, such as the American ERNi- or ERNiCr- designations, so check that class against the maker's data sheet and the specification or procedure for your job. If you are joining two different metals, the filler needs to suit both.

    How should I prepare nickel alloy before welding?icon-minus-redicon-plus-red

    Degrease the joint area first, remove the surface oxide by machining, grinding or a similar method, and then degrease again to remove anything introduced during cleaning. Wire brushing alone is usually not enough, because it tends to polish the oxide rather than remove it.

    Between passes, remove oxide as well, as it can cause inclusions and lack of fusion. Weld soon after cleaning, and keep the cleaning tools dedicated to nickel alloys.

    Which shielding gas should I use for TIG welding nickel alloys?icon-minus-redicon-plus-red

    Pure argon is the usual choice, and argon with helium or with a small addition of hydrogen is also used for some alloys. A hydrogen addition can improve the fluidity of the weld pool and give cleaner welds, but it is not suitable for every alloy, so check the filler maker's recommendation.

    Good gas coverage matters, because oxygen and nitrogen from the air cause porosity. Keep gas hoses in good condition, avoid draughts, and use a back purge where the root side of the joint needs protecting.

    Why does a nickel filler get used to join stainless steel to carbon steel?icon-minus-redicon-plus-red

    Nickel alloy fillers generally perform well in dissimilar joints between ferritic and austenitic steels. The thermal expansion of nickel alloys sits between that of ferritic steel and austenitic stainless steel, so the joint suffers less thermal fatigue when it heats and cools repeatedly.

    The right nickel filler for a dissimilar joint depends on the metals and the service conditions, such as temperature and corrosion. Check the filler maker's data sheet and, for critical work, the specification you are working to.