    Bohler Union AlMg 4.5Mn 5183, 1.2mm MIG Wire, 7Kg Reel, ER5183
    26261

    £126.69  EX VAT
    SSP Suggested Selling Price = £147.00  YOU SAVE £20.31
     Buy in 3 easy interest free payments of £42.23† with

    Solid wire for GMAW and GTAW of AlMg alloys. The weld metal is resistant to seawater. Base material should be cleaned near the seam. Pre-heating 150°C for plates > 15mm.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Mig 5183 FAQs

    Straight answers to the questions people ask most when choosing and using 5183 aluminium MIG wire.

    Which base alloys is 5183 normally used on?icon-minus-redicon-plus-red

    It is mostly used on the higher-magnesium 5000 series alloys such as 5083, 5086 and 5456, and sometimes on lower-magnesium 5000 series material such as 5052. It is not normally chosen for 1000, 3000 or 6000 series alloys, where other fillers give better results.

    Parent alloy, temper, thickness and service conditions all influence the filler choice, so check a filler selection chart and your welding procedure rather than relying on the alloy number alone.

    Can I use 5183 for parts that run hot?icon-minus-redicon-plus-red

    Generally no. Aluminium-magnesium fillers with more than about 3 per cent magnesium, including 5183, can become prone to stress corrosion cracking if the weld sees service temperatures above about 65 degrees C for long periods, especially in a corrosive environment such as salt water.

    For parts that stay warm in service, a lower-magnesium filler is the usual alternative, although it gives lower strength. Check the maker's data sheet and the governing specification for your application.

    Why does aluminium wire feed badly, and how do I fix it?icon-minus-redicon-plus-red

    Aluminium wire is soft, so it is easily crushed, scraped or tangled in the cable, which causes erratic feeding and the wire bunching at the drive rolls (often called bird-nesting). Use U-groove or soft V-groove drive rolls, lower the roll pressure than you would use for steel, and fit a plastic liner such as nylon or PTFE instead of a steel one, which can scratch the wire and shed fine shavings.

    Keep the cable short and straight, make sure the contact tip suits aluminium, and keep the liner clean. A guide tube between the rolls and the liner also helps.

    Do I need a push-pull gun or spool gun?icon-minus-redicon-plus-red

    Not always. A standard push feed system can handle aluminium, particularly with larger wire diameters and a short torch cable. Thin, soft wire is harder to push, and long cable runs make it worse.

    A push-pull torch, with a motor in the handle to help pull the wire, or a spool gun that carries a small spool of wire on the torch, makes feeding more reliable on thinner wire and longer reaches. 5183 is a little stiffer than the softest aluminium wires, but the same advice applies. Check what your machine supports.