    • ER-NiCrMo-4 is used for the welding of alloys that have similar chemical compositions, this includes dissimilar materials of nickel-base alloys, steels and stainless steels.
    • Due to the high molybdenum content, this alloy offers excellent resistance against stress & corrosion cracking, pitting and crevice corrosion.
    • Typically used on pipelines, pressure vessels, chemical processing plants, offshore oil platforms, gas facilities, power generation and marine environments etc.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    High Nickel TIG Wire FAQs

    Straight answers to the questions people ask most when choosing and using nickel alloy TIG filler wire.

    How do I choose the right nickel alloy TIG filler?icon-minus-redicon-plus-red

    Start from the base metal. For most nickel alloys the filler is chosen to match the parent metal, for example a pure nickel rod for commercial purity nickel and a nickel-chromium-molybdenum rod for the matching alloy 625 type. Many fillers contain small additions such as titanium, aluminium or niobium to reduce porosity and cracking.

    The filler is named by its class, such as the American ERNi- or ERNiCr- designations, so check that class against the maker's data sheet and the specification or procedure for your job. If you are joining two different metals, the filler needs to suit both.

    Why does cleanliness matter so much with nickel alloys?icon-minus-redicon-plus-red

    Nickel alloys are easily embrittled at high temperature by sulphur, lead, phosphorus, boron and bismuth. These can come from oils, grease, cutting fluids, paints, marker pens and temperature-indicating crayons. Contamination of this kind can cause cracking in the weld or heat-affected zone.

    Keep the joint, the filler wire and your tools free of these materials, and use brushes and tools kept only for nickel alloys. Avoid marking with ordinary markers or crayons near the weld.

    How should I prepare nickel alloy before welding?icon-minus-redicon-plus-red

    Degrease the joint area first, remove the surface oxide by machining, grinding or a similar method, and then degrease again to remove anything introduced during cleaning. Wire brushing alone is usually not enough, because it tends to polish the oxide rather than remove it.

    Between passes, remove oxide as well, as it can cause inclusions and lack of fusion. Weld soon after cleaning, and keep the cleaning tools dedicated to nickel alloys.

    What is the best technique for welding nickel alloys?icon-minus-redicon-plus-red

    Nickel alloys do not flow like mild steel, so the weld does not wet out sideways much. Use stringer beads with little weaving, keep the heat input modest and aim for a slightly convex bead profile. Heat input and interpass temperature limits depend on the alloy, so follow the filler maker's guidance.

    Grind out the start and stop points of each run to avoid porosity. Higher current does not usually give deeper penetration, and a joint preparation with a wide enough angle helps you reach the root.