WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : ED022061  

    Lincoln Electric Lincore 15CrMn, 2.8mm Hardfacing Flux Cored MIG Wire, 22.7Kg Reel, MF7-GF-250-KP
    ED022061

    £406.71  EX VAT
    SSP Suggested Selling Price = £508.39  YOU SAVE £101.68
     Buy in 3 easy interest free payments of £135.57† with

    Provides an austenitic manganese deposit which exhibits very good crack resistance. Work hardens for overlay or joining austenitic manganese steel to itself or carbon steel. Can be used as a build-up layer before capping with abrasion-resistant alloys. Can be used in open arc mode for joining austenitic manganese steel to carbon steel, low alloy steel, austenitic manganese steel, or stainless steel. Unlimited layers with proper preheat and interpass temperatures and procedures.

    Typical Applications
    Spreader Cones
    Crusher Hammers
    Austenitic manganese parts

    Welding Positions
    Flat and Horizontal

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Hard Facing MIG Wire FAQs

    Straight answers to the questions buyers ask most when choosing and using hardfacing cored wire for wear-resistant overlays.

    How do I choose the right hardfacing wire for my wear problem?icon-minus-redicon-plus-red

    Start by working out how the part wears. Sliding of loose material under low pressure (low-stress abrasion) usually calls for a harder deposit with plenty of carbides. Crushing and grinding under high pressure needs a tougher deposit with well-spread carbides. Heavy pounding or gouging usually points to a work-hardening austenitic manganese type, and metal-to-metal wear or galling suits a tool-steel type of deposit.

    Most real parts suffer a mix of wear types, so aim for the best balance rather than the hardest deposit. Check the base metal too, because it affects preheat and whether a buffer layer is needed. Our team can help you match a wire to the job.

    What is the difference between chromium carbide, martensitic and manganese hardfacing wires?icon-minus-redicon-plus-red

    Chromium carbide deposits are the usual choice for abrasion with low to moderate impact. They are very hard but brittle, so they tend to show fine cracks and are usually limited in how many layers can be built up.

    Martensitic deposits are a compromise: good abrasion resistance with better toughness, so they suit mixed abrasion and impact, and they are often used as a build-up as well. Austenitic manganese deposits are tough and harden under hammering, so they suit heavy impact and rebuilding manganese steel parts, but they are not the best choice for pure sliding abrasion. Always check the maker's data sheet for the alloy you are considering.

    Do I need a buffer layer before hardfacing?icon-minus-redicon-plus-red

    Often, yes. A buffer or build-up layer gives the hard deposit a tough, crack-resistant base, and it is commonly used on steels that harden easily and when rebuilding worn parts. The buffer must be compatible with both the base metal and the final hardfacing alloy.

    On manganese steel, an austenitic buffer is normally used rather than a carbon steel build-up. Before welding, remove the old work-hardened surface from manganese steel, because leaving it in place can cause cracking under the weld. If a wire's data sheet specifies a buffer layer for your base metal, follow it.

    How many layers of hardfacing can I put on?icon-minus-redicon-plus-red

    It depends on the alloy, the base metal and the process. The first layer is diluted most by the base metal, so its hardness is usually lower than the data sheet value, and two or three layers are often needed to reach the quoted hardness. Chromium carbide types are normally limited in the number of layers because of cracking, while manganese types can usually be built up further unless the maker says otherwise.

    On high-carbon steels the number of layers is often limited because of cracking risk. Check the data sheet for the maximum layer count and overall thickness for the wire you are using.

    Shop Similar Categories