    SIFSteel A33 Steel TIG Wire, 1000mm Cut Lengths - AWS A5.28 ER90S-B3, 5Kg Pack
    RA33XX50

    Select Option 
    Prices From £75.52 ex VAT

    A copper-coated alloy steel rod containing 2.5% chromium, and 1.0% molybdenum.  It is suitable for high-temperature and pressure applications on materials of similar composition.  It is used in the chemical industry and in the ammonia synthesis process, for heat exchangers, boilers, piping and pressure vessels for temperature service up to about 600°c.  It will also find applications in the petro-chemical industries, suitable for facing on casting and for casting repairs.

    BS: 2901 A33, AWS ER90S-B3
    Metal Composition Melting*C U.T.M N/mm² Hardness BHN
    0.1 C, 0.5 Si, 1 Mn, 2.4 Cr, 1 Mo 1450 525 200

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig Er90S-B3 FAQs

    Straight answers to the questions people ask most when choosing and using 2.25Cr-1Mo chromium-molybdenum TIG filler wire.

    What is ER90S-B3 TIG wire used for?icon-minus-redicon-plus-red

    ER90S-B3 is a low-alloy chromium-molybdenum solid rod, classed under the American standard for low-alloy steel filler rods. It contains roughly 2.25% chromium and 1% molybdenum, and it is used to weld creep-resistant steels of the same type, such as P22 pipe and 2.25Cr-1Mo plate used in power plant, refinery pipework and pressure vessels.

    The chromium and molybdenum help the weld keep its strength at high service temperatures. It is not a general-purpose steel rod, so use it where the drawing, code or welding procedure calls for a matching 2.25Cr-1Mo filler.

    Which base metals does it match, and what about dissimilar joints?icon-minus-redicon-plus-red

    It is chosen to match 2.25Cr-1Mo steels, for example P22 pipe and the equivalent plate grades. Other creep-resistant steels have their own matching fillers, so do not assume one rod fits them all.

    For dissimilar joints, the filler normally matches the less highly alloyed of the two steels, but the final choice should come from your qualified welding procedure and the applicable code. If you are unsure, check with your welding engineer before buying.

    Does the weld need post-weld heat treatment?icon-minus-redicon-plus-red

    Almost always. Post-weld heat treatment is mandatory in most application codes for creep-resistant steels. It softens the hard as-welded structure, improves toughness and sets up the carbide structure needed for long-term creep strength. The temperature and hold time come from the procedure and code, so do not take figures from a rod description.

    Plan the heat treatment before you start welding, because it affects when the joint can be released and inspected.

    Why do data sheets for this wire quote an X factor or low impurity levels?icon-minus-redicon-plus-red

    In 2.25Cr-1Mo weld metal, trace impurities such as phosphorus, tin, antimony and arsenic can gather at grain boundaries during long periods in the 400 to 600 degrees C range. This is called temper embrittlement, and it makes the weld less tough. The X factor is a calculation from these impurities, and a lower figure means lower risk.

    A low-impurity wire with a stated X factor limit is therefore chosen for pressure equipment that will run hot for years. If your specification sets a limit, check the wire's certificate to confirm it meets it.