    • ER-Ni1 is used for the welding and cladding of Nickel 200 and Nickel 201 alloys.
    • Perfect for joining Monel alloys and copper-nickel alloys to carbon steels.
    • Ni1 contains enough titanium to control the weld-metal porosity on welding processes.
    • Typically used in the chemical processing industries, synthetic fibre production & food processing equipment etc.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    High Nickel TIG Wire FAQs

    Straight answers to the questions people ask most when choosing and using nickel alloy TIG filler wire.

    How do I choose the right nickel alloy TIG filler?icon-minus-redicon-plus-red

    Start from the base metal. For most nickel alloys the filler is chosen to match the parent metal, for example a pure nickel rod for commercial purity nickel and a nickel-chromium-molybdenum rod for the matching alloy 625 type. Many fillers contain small additions such as titanium, aluminium or niobium to reduce porosity and cracking.

    The filler is named by its class, such as the American ERNi- or ERNiCr- designations, so check that class against the maker's data sheet and the specification or procedure for your job. If you are joining two different metals, the filler needs to suit both.

    Which shielding gas should I use for TIG welding nickel alloys?icon-minus-redicon-plus-red

    Pure argon is the usual choice, and argon with helium or with a small addition of hydrogen is also used for some alloys. A hydrogen addition can improve the fluidity of the weld pool and give cleaner welds, but it is not suitable for every alloy, so check the filler maker's recommendation.

    Good gas coverage matters, because oxygen and nitrogen from the air cause porosity. Keep gas hoses in good condition, avoid draughts, and use a back purge where the root side of the joint needs protecting.

    What is the best technique for welding nickel alloys?icon-minus-redicon-plus-red

    Nickel alloys do not flow like mild steel, so the weld does not wet out sideways much. Use stringer beads with little weaving, keep the heat input modest and aim for a slightly convex bead profile. Heat input and interpass temperature limits depend on the alloy, so follow the filler maker's guidance.

    Grind out the start and stop points of each run to avoid porosity. Higher current does not usually give deeper penetration, and a joint preparation with a wide enough angle helps you reach the root.

    Why does a nickel filler get used to join stainless steel to carbon steel?icon-minus-redicon-plus-red

    Nickel alloy fillers generally perform well in dissimilar joints between ferritic and austenitic steels. The thermal expansion of nickel alloys sits between that of ferritic steel and austenitic stainless steel, so the joint suffers less thermal fatigue when it heats and cools repeatedly.

    The right nickel filler for a dissimilar joint depends on the metals and the service conditions, such as temperature and corrosion. Check the filler maker's data sheet and, for critical work, the specification you are working to.