WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : ED03113  

    Lincoln Electric Lincore 60-O, Hardfacing Flux Cored MIG Wire, 11.34Kg Reel, MF10-GF-60-CG
    ED03113

    Select Option 
    Prices From £360.70 ex VAT

    Deposits feature higher alloy levels to resist both abrasion and moderate impact. Can be used at temperatures up to 704°C (1300°F). To be used on carbon, low alloy, manganese and stainless steels and cast iron. Deposit is limited to two layers.

    Typical Applications
    Bucket lips
    Crusher hammers
    Ore chutes
    Dozer blades
    Ripper teeth

    Welding Positions
    Flat and Horizontal

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Hard Facing MIG Wire FAQs

    Straight answers to the questions buyers ask most when choosing and using hardfacing cored wire for wear-resistant overlays.

    What is the difference between chromium carbide, martensitic and manganese hardfacing wires?icon-minus-redicon-plus-red

    Chromium carbide deposits are the usual choice for abrasion with low to moderate impact. They are very hard but brittle, so they tend to show fine cracks and are usually limited in how many layers can be built up.

    Martensitic deposits are a compromise: good abrasion resistance with better toughness, so they suit mixed abrasion and impact, and they are often used as a build-up as well. Austenitic manganese deposits are tough and harden under hammering, so they suit heavy impact and rebuilding manganese steel parts, but they are not the best choice for pure sliding abrasion. Always check the maker's data sheet for the alloy you are considering.

    Do I need to preheat before hardfacing?icon-minus-redicon-plus-red

    It depends on the base metal. Higher-carbon and low-alloy steels, tool steels, martensitic stainless steels and most cast irons are normally preheated, and the amount depends on the carbon and alloy content, the thickness and the wire. Preheating also helps reduce distortion and cracking, and slow cooling afterwards helps protect the heat-affected zone.

    Austenitic manganese steel is different. It should not be preheated much and should not be allowed to get too hot, because excessive heat makes it brittle, so keep the base metal below the maximum temperature the maker gives. Always follow the wire maker's data sheet and your welding procedure.

    Is it normal for a hardfacing deposit to crack?icon-minus-redicon-plus-red

    With chromium carbide types, fine cracks running across the beads (check cracking) are usually normal. They form as the hard, brittle deposit cools and contracts, and they relieve stress. They are generally not harmful to wear performance unless the part sees a corrosive service.

    Cracks that run along the bead, or that go down into the base metal (underbead cracking), are a warning sign. They can lead to the deposit breaking away. Common causes are too little dilution with the base metal, no buffer layer, too little preheat or cooling too quickly. If your deposit shows irregular cracking, review the procedure and the data sheet.

    How many layers of hardfacing can I put on?icon-minus-redicon-plus-red

    It depends on the alloy, the base metal and the process. The first layer is diluted most by the base metal, so its hardness is usually lower than the data sheet value, and two or three layers are often needed to reach the quoted hardness. Chromium carbide types are normally limited in the number of layers because of cracking, while manganese types can usually be built up further unless the maker says otherwise.

    On high-carbon steels the number of layers is often limited because of cracking risk. Check the data sheet for the maximum layer count and overall thickness for the wire you are using.

    Shop Similar Categories