WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : 60111006XX  

    Nickel Alloy 825 TIG Wire, 1000mm Cut Lengths - AWS A5.14 ER NiFeCr-1, 5Kg Pack
    60111006XX

    Select Option 
    Prices From £248.00 ex VAT

    • Alloy 825 is a nickel-iron-chromium wire making this a suitable choice for a variety of difficult applications.
    • This wire provides high levels of corrosion resistance to both moderately oxidising and reducing environments.
    • Perfect for overlay cladding where similar chemical composition is required.
    • Excellent weldability with fully austenitic weld metal with high resistance against stress corrosion cracking in media containing chloride ions.
    • Typically used in the chemical processing industries, petrochemical, paper manufacturing and power generation etc.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    High Nickel TIG Wire FAQs

    Straight answers to the questions people ask most when choosing and using nickel alloy TIG filler wire.

    How should I prepare nickel alloy before welding?icon-minus-redicon-plus-red

    Degrease the joint area first, remove the surface oxide by machining, grinding or a similar method, and then degrease again to remove anything introduced during cleaning. Wire brushing alone is usually not enough, because it tends to polish the oxide rather than remove it.

    Between passes, remove oxide as well, as it can cause inclusions and lack of fusion. Weld soon after cleaning, and keep the cleaning tools dedicated to nickel alloys.

    Which shielding gas should I use for TIG welding nickel alloys?icon-minus-redicon-plus-red

    Pure argon is the usual choice, and argon with helium or with a small addition of hydrogen is also used for some alloys. A hydrogen addition can improve the fluidity of the weld pool and give cleaner welds, but it is not suitable for every alloy, so check the filler maker's recommendation.

    Good gas coverage matters, because oxygen and nitrogen from the air cause porosity. Keep gas hoses in good condition, avoid draughts, and use a back purge where the root side of the joint needs protecting.

    What is the best technique for welding nickel alloys?icon-minus-redicon-plus-red

    Nickel alloys do not flow like mild steel, so the weld does not wet out sideways much. Use stringer beads with little weaving, keep the heat input modest and aim for a slightly convex bead profile. Heat input and interpass temperature limits depend on the alloy, so follow the filler maker's guidance.

    Grind out the start and stop points of each run to avoid porosity. Higher current does not usually give deeper penetration, and a joint preparation with a wide enough angle helps you reach the root.

    Why does a nickel filler get used to join stainless steel to carbon steel?icon-minus-redicon-plus-red

    Nickel alloy fillers generally perform well in dissimilar joints between ferritic and austenitic steels. The thermal expansion of nickel alloys sits between that of ferritic steel and austenitic stainless steel, so the joint suffers less thermal fatigue when it heats and cools repeatedly.

    The right nickel filler for a dissimilar joint depends on the metals and the service conditions, such as temperature and corrosion. Check the filler maker's data sheet and, for critical work, the specification you are working to.

    Shop Similar Categories