WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : TER90SB3-24  

    Lincoln ER90S-B3 2.4mm Diameter Low Alloy Tig Wire, 5kg Pack
    TER90SB3-24

    £101.08  EX VAT
    SSP Suggested Selling Price = £126.35  YOU SAVE £25.27
     Buy in 3 easy interest free payments of £33.69† with

    Copper-coated wire for TIG and MIG welding 2¼Cr-1Mo creep-resisting steels, conforming to the AWS/ASME specification.

    Applications
    These consumables are designed for prolonged elevated temperature service up to 600°C. The main areas of application are associated with a steam-generating power plant, e.g. piping, turbine castings, steam chests, valve bodies and boiler superheaters. Some of the consumables will also find service in refineries where they are used for corrosion resistance to sulphur-bearing crude oil at 250-450°C. Some of the consumables will also find applications in the chemical and petrochemical industries where they are used for resistance to hydrogen attack in the fabrication of hydrocrackers, coal liquefaction plants and NH3 pressure vessels operating at up to 450°C. In the as-welded condition, the consumables also provide a useful source of 300HV hardness weld deposit for build-up or hard surfacing to resist metal-to-metal wear, heavy impact and the repair of P20 mould steel.

    Specification
    AWS A5.28: ER90S-B3 BS EN ISO 21952-B: 2C1M

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Related Items

    Tig Er90S-B3 FAQs

    Straight answers to the questions people ask most when choosing and using 2.25Cr-1Mo chromium-molybdenum TIG filler wire.

    What is ER90S-B3 TIG wire used for?icon-minus-redicon-plus-red

    ER90S-B3 is a low-alloy chromium-molybdenum solid rod, classed under the American standard for low-alloy steel filler rods. It contains roughly 2.25% chromium and 1% molybdenum, and it is used to weld creep-resistant steels of the same type, such as P22 pipe and 2.25Cr-1Mo plate used in power plant, refinery pipework and pressure vessels.

    The chromium and molybdenum help the weld keep its strength at high service temperatures. It is not a general-purpose steel rod, so use it where the drawing, code or welding procedure calls for a matching 2.25Cr-1Mo filler.

    Which base metals does it match, and what about dissimilar joints?icon-minus-redicon-plus-red

    It is chosen to match 2.25Cr-1Mo steels, for example P22 pipe and the equivalent plate grades. Other creep-resistant steels have their own matching fillers, so do not assume one rod fits them all.

    For dissimilar joints, the filler normally matches the less highly alloyed of the two steels, but the final choice should come from your qualified welding procedure and the applicable code. If you are unsure, check with your welding engineer before buying.

    How does ER90S-B3 differ from ER80S-B2 and ER90S-B9?icon-minus-redicon-plus-red

    The difference is mainly the chromium and molybdenum content, which sets the base metal each one matches. ER80S-B2 is a lower-alloy wire (about 1.25% chromium, 0.5% molybdenum) for steels such as P11. ER90S-B3 steps up to about 2.25% chromium and 1% molybdenum for P22. ER90S-B9 is in a different class altogether, with about 9% chromium, for P91-type steels.

    They are not interchangeable. Using a lower-alloy filler on P22, or the reverse, is generally not accepted on code work without engineering approval.

    Do I need to preheat before welding with it?icon-minus-redicon-plus-red

    Yes. Chromium-molybdenum creep-resistant steels are prone to hydrogen cracking, so preheat is normally essential, and the interpass temperature is kept below a set maximum. The minimum preheat usually rises with thickness.

    The correct figures for your job depend on thickness, joint and the code, so always follow your qualified welding procedure. Keep the joint at temperature between passes, and do not let it cool to room temperature part-way through unless the procedure allows it.

    Shop Similar Categories