WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : 6011100XXX  

    Nickel Alloy C22 TIG Wire, 1000mm Cut Lengths - AWS A5.14 ER NiCrMo-10, 5Kg Pack
    6011100XXX

    Select Option 
    Prices From £441.75 ex VAT
    • Nickel-chromium-molybdenum alloy designed for joining C22, 625, 825 or combinations of these alloys.
    • Provides a tough Nb-free weld metal for dissimilar welds in super austenitic and super duplex stainless steels.
    • Offers excellent resistance against stress & corrosion cracking, pitting and crevice corrosion.
    • Extensively used for overlays and cladding of lower alloy steels.
    • Typically used in the welding of aggressively corrosive media in chemical processing plants, corrosion resistant overlays and in severe offshore and petrochemical environments etc.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    High Nickel TIG Wire FAQs

    Straight answers to the questions people ask most when choosing and using nickel alloy TIG filler wire.

    Why does cleanliness matter so much with nickel alloys?icon-minus-redicon-plus-red

    Nickel alloys are easily embrittled at high temperature by sulphur, lead, phosphorus, boron and bismuth. These can come from oils, grease, cutting fluids, paints, marker pens and temperature-indicating crayons. Contamination of this kind can cause cracking in the weld or heat-affected zone.

    Keep the joint, the filler wire and your tools free of these materials, and use brushes and tools kept only for nickel alloys. Avoid marking with ordinary markers or crayons near the weld.

    How should I prepare nickel alloy before welding?icon-minus-redicon-plus-red

    Degrease the joint area first, remove the surface oxide by machining, grinding or a similar method, and then degrease again to remove anything introduced during cleaning. Wire brushing alone is usually not enough, because it tends to polish the oxide rather than remove it.

    Between passes, remove oxide as well, as it can cause inclusions and lack of fusion. Weld soon after cleaning, and keep the cleaning tools dedicated to nickel alloys.

    What is the best technique for welding nickel alloys?icon-minus-redicon-plus-red

    Nickel alloys do not flow like mild steel, so the weld does not wet out sideways much. Use stringer beads with little weaving, keep the heat input modest and aim for a slightly convex bead profile. Heat input and interpass temperature limits depend on the alloy, so follow the filler maker's guidance.

    Grind out the start and stop points of each run to avoid porosity. Higher current does not usually give deeper penetration, and a joint preparation with a wide enough angle helps you reach the root.

    Why does a nickel filler get used to join stainless steel to carbon steel?icon-minus-redicon-plus-red

    Nickel alloy fillers generally perform well in dissimilar joints between ferritic and austenitic steels. The thermal expansion of nickel alloys sits between that of ferritic steel and austenitic stainless steel, so the joint suffers less thermal fatigue when it heats and cools repeatedly.

    The right nickel filler for a dissimilar joint depends on the metals and the service conditions, such as temperature and corrosion. Check the filler maker's data sheet and, for critical work, the specification you are working to.