    Gullco Flux Holding Hopper. 115 Volt, 100-400°F (38-205°C) Temperature, 400 Watts, Complete with Thermostat & Thermometer. 44Kg Capacity
    GOV-100-FH

    £823.00  EX VAT
     Buy in 3 easy interest free payments of £274.33† with

    This 100lb Capacity Flux Hopper is designed for mounting either directly above the welding head or on the welding manipulator to maintain the flux in its original dry state. It is complete with mountings lugs, a lift-off loading lid, a thermometer, a flux level window, a flux screen and a flux heating system incorporating 40 watts of low-density elements. A thermostat controls the temperature. The temperature range is 38 - 205°C (100° to 400°F). For operation on 115 volts. Weight 12Kg. Dimensions: 572mm H x 330mm W x 279mm D.

    Product Details

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Flux Ovens FAQs

    Answers to common questions about holding ovens and heated hoppers for submerged arc welding flux.

    Why does submerged arc flux have to be kept dry?icon-minus-redicon-plus-red

    Flux that has taken up moisture releases hydrogen into the weld pool when it melts in the arc. Moisture in the flux or electrode coating is the principal source of hydrogen in flux-based welding. Hydrogen in the weld can lead to delayed cracking, especially in higher-strength steels, and damp flux is also a known cause of porosity.

    Keeping flux dry from the packet to the weld is therefore part of controlling weld quality. The flux maker's data sheet and your welding procedure set out how dry it needs to be for the job.

    Do all submerged arc fluxes absorb moisture in the same way?icon-minus-redicon-plus-red

    No. Fused fluxes are made by melting and crushing, and are resistant to moisture pick-up. Agglomerated (bonded) fluxes are made from a baked wet mix with binders that attract moisture, so moisture pick-up can be a problem on the shop floor and baking before use may be needed.

    This is why the type of flux affects how you store and handle it. Check the flux packaging and data sheet for the type and the maker's handling rules, and ask our team if you are unsure which oven arrangement suits your flux.

    Do I need an oven if my flux comes in sealed packaging?icon-minus-redicon-plus-red

    Not always. Some suppliers now pack flux in airtight packaging, which is designed to let it be used straight from the pack at low hydrogen levels without baking first. Once the pack is opened, though, the flux is exposed to the air and that protection stops.

    If you use the whole pack quickly, an oven may not be needed. If opened flux sits in the hopper or is put back into storage, a holding oven or heated hopper is a sensible way to keep it dry. Follow the flux maker's instructions and your welding procedure for how long opened flux may be left.

    Can compressed air used for flux recovery affect the flux?icon-minus-redicon-plus-red

    Yes. Flux recovery units driven by compressed air can carry moisture and oil into the recovered flux if the air is not dry and clean. Compressed air used with a flux recovery unit should be thoroughly dried.

    A damp or oily recirculating flux can cause porosity, even if it was dry in the oven. Drain the air line and filters regularly, and follow the recovery unit maker's instructions. Keep the recycled flux separate from any contaminated or wet flux.